Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 28.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 28.0 GPa
4060 ksi
ISO 527
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c..
Tensile Modulus 28.0 GPa
4060 ksi
ISO 527
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced
General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex.
Tensile Modulus 28.0 GPa

@Temperature 23.0 °C
4060 ksi

@Temperature 73.4 °F
ISO 527
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont..
Tensile Modulus 28.0 GPa

@Temperature 23.0 °C
4060 ksi

@Temperature 73.4 °F
ISO 527
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com..
Tensile Modulus 28.0 GPa

@Temperature 23.0 °C
4060 ksi

@Temperature 73.4 °F
ISO 527
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, ..
Tensile Modulus 28.0 GPa
4060 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Stat-kon EE008E PEI
LNP STAT-KON* EE008E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas r..
Tensile Modulus 28.0 GPa
4060 ksi
ISO 527
Vyncolit X655 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent dimensional stability and a very low coefficient of thermal expansion. UL listed.USES: Automotive disc brake pistons and gask..
Tensile Modulus 28.0 GPa
4060 ksi
ISO 527-1
Vyncolit X655/1 Glass Fiber and Mineral Filled Novolac Phenolic
Novolac resin based, glass fiber and mineral filled. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in particular in the ABS system..
Tensile Modulus 28.0 GPa
4060 ksi
90º, RT, Dry; EN2561
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 54%/G1088 Glass/Carbon Fiber
Information provided by HexCel
Tensile Modulus 28.0 GPa

@Temperature 75.0 °C
4060 ksi

@Temperature 167 °F
Wet; EN2561
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber
Information provided by HexCel
Tensile Modulus 28.0 GPa
4060 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® GC-4H PA*-CF40
Product description: Grivory GC-4H is a 40% carbon-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamide. Grivo..
Tensile Modulus 28.0 GPa
4060 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® GVX-7 H black 9915 PA*-GF70
Product description: Grivory GVX-7H black 9915 is a 70% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam..
Tensile Modulus 28.0 GPa
4060 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® GVX-7 H nat PA*-GF70
Product description: Grivory GVX-7H natural is a 70% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid..
Tensile Modulus 28.0 GPa
4060 ksi
ISO 527
Eurotec® Tecomid® NAX0 GR70 NL HS PA6.6, 70% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Copyright © lookpolymers.com All Rights Reserved