Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | ISO 180/1A |
NOVA Chemicals DYLARK® 378 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | Result based on similar products; ISO 180/A |
Victrex® PEEK 600PF Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact complian.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | ISO 180 |
LNP Stat-Kon® LC-1003 Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | ISO 180/A |
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | ISO 180/A |
Victrex® PEEK 650P PolyEtherEtherKetone High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, coarse powder for extrusion compounding, low flow, FDA food contact compliant, color natural.Info.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | Volume Resistivity 10.5 [log{ohm-cm)] |
TIMCAL ENSACO™ 350G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® T-731E-BK 10% Reinforced Abrasion Resistant Nylon 6 Description: Abrasion Resistant Nylon 6Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² @Temperature -20.0 °C |
3.57 ft-lb/in² @Temperature -4.00 °F |
ASTM D256 |
C.O.I.M. LARIPUR® LPR70D60 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | ISO 179/1eA |
BLUESTAR PBT 6630 30% Glass Filled PBT6630 is an injection molding grade, with 30% glass fiber reinforced, high heat stability, and electrical properties, easy to process. It is widely used in automotive, home appliance, E/E industry.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | ISO 180/1A |
Addiplast Addilene H 511 V30 Polypropylene Homopolymer Glass fiber reinforced, high modulus and improved stiffnessInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | ISO 180 |
Total PPR 3260 Random Copolymer Polypropylene, Extrusion Grade Polypropylene PPR 3260 is a random copolymer polypropylene with a melt flow index of 1.8 g/10 min suitable for extrusion applications.Information provided by Total Petrochemicals. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL BK039 is a 13 % glass reinforced heat stabilized lubricated slightly toughened black polyamide 66 for injection molding. It.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® ST45G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed by in.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | ISO 180/1A |
Addiplast Addilene J 326 V30 Polypropylene Copolymer High modulus, high durabilityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl B2 ZV15 Nylon 6, 15% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |