Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Europe-Africa-Middle East)
Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and ..
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ISO 294-4
Celanese Celanex® 6402R PBT, 40% Mineral / Glass Reinforced  (Unverified Data**)
Celanex 6402R is a 40% Glass/ mineral filled polyester with 25% Post Consumer Recycled content. It is available in natural, black and various colors including metallic colors.40% Glass/Mineral with..
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ASTM D955
LNP Lubricomp® EFL-4036 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
Measured on 102 mm X 102 mm X 3.2 mm Plaques, Edge Gated
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide Compound  (Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® BR42B is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surf..
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
Measured on 102 mm X 102 mm X 3.2 mm Plaques, Edge Gated
Chevron Phillips Ryton® BR42C Polyphenylene Sulfide Compound  (discontinued **)
Black Polyphenylene Sulfide CompoundRyton® BR42C is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surface fric..
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ISO 294-4
Mitsubishi Xantar® G4F 25 R Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
Kuraray Genestarâ„¢ GP2450NH-2 Nylon, 45% Glass Filled
Standard V-0 Grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm.This grade meets UL94, V-0..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
LATI Latamid 6 H2 G/55 PA 6, 55% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0075 cm/cm
0.0050 - 0.0075 in/in
LATI Laticonther 87/28 GR/50 PC, 50% Graphite Reinforced
High thermal conductivity product based on Polycarbonate (PC). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0080 cm/cm

@Time 86400 sec
0.0050 - 0.0080 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP ZFL24 PPE+PS
LNP* LUBRICOMP* ZFL24 is a compound based on PPE+PS resin containing 20% Glass Fiber, 10% PTFE. Added feature of this grade is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0080 cm/cm

@Time 86400 sec
0.0050 - 0.0080 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Lubricomp ZFL24 PPO
LNP* Lubricomp* ZFL24 is a compound based on Modified Polyphenylene Oxide (PPO) containing glass fiber and PTFE lubricant. Characteristics of this grade are: Internally Lubricated.This data was su..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics ULTEM AUT230 PEI (Europe-Africa-Middle East)
Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of..
Linear Mold Shrinkage, Transverse 0.0050 cm/cm

@Thickness 3.20 mm
0.0050 in/in

@Thickness 0.126 in
ASTM D955
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® V9260CS PET (Asia Pacific)
Color Stable Glass filled PET
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon OEL36A PPS
LNP* Stat-Kon* OEL36A is a compound based on Polyphenylene Sulfide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This ..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Asia Pacific)
PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-loy AX06484X ABS
LNP* Stat-Loy* AX06484 is a compound based on ABS resin containing mineral filler. Characteristics of this grade is it is extrudeable and static dissipative.This data was supplied by SABIC-IP for t..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0056 cm/cm

@Time 86400 sec
0.0050 - 0.0056 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP NX10302 PC+ABS (Asia Pacific)
This is a PC/ABS compound with improved plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0090 cm/cm
0.0050 - 0.0090 in/in
ASTM D955
Shinkong Synthetic Fibers Shinite® D202G15 PBT, 15% Glass Filled, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0090 cm/cm
0.0050 - 0.0090 in/in
ISO DIS 294-4
Wellman Wellamid® GF13-66 22LH-NBK1 13% Glass Fiber Reinforced, General Purpose Nylon 66
Description: Glass Fiber Reinforced, General Purpose Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0060 cm/cm
0.0050 - 0.0060 in/in
ASTM D955
Lubrizol Pellethane® 2363-90AE Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® LBV-30H FWA black 9225 PA12-GF30
Product Description: Grilamid LBV-30H FWA black 9225 is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined wit..
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® BGZ-40 PA6-GF40
Product description: Grilon BGZ-40 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 40% glass fibers. Grilon BGZ-40 has the following important properties:..
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® HT1V-5 FWA black 9225 PA6T/6I-GF50
Product description: Grivory HT1V-5 FWA black 9225 is a 50 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: ..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ISO 294-4
Celanese Celanex® 6500HF PBT, Mineral / Glass Reinforced
6500HF is a high flow, 30% glass/mineral filled polybutylene terephthalate (PBT) with improved warp resistance and surface smoothness.Information provided by Celanese Corporation.
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
Advanced Polymer Alloys DuraGrip™ 6160 BK Melt Processable Elastomer
DuraGrip™ 6160BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6160BK has an excellent soft touch feel a..
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY
Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding. T..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP JF004L PES
LNP* THERMOCOMP* JF004L is a compound is based on Polyethersulfone containing 20% Glass Fiber. Characteristics of this grade is: Low Extractible