Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Mold Temperature = 410 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 193 - 210 °C
379 - 410 °F
Blow Molding
PolyOne Geon™ Vinyl Packaging VB7 White 215 Polyvinyl Chloride, Rigid (PVC, Rigid)
A rigid PVC Compound designed for extrusion blow molding balusters for railings.Information provided by PolyOne
Mold Temperature 193 - 210 °C
379 - 410 °F
Blow Molding
PolyOne Geon™ Vinyl Packaging VEO-184 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Mold Temperature 175 - 210 °C
347 - 410 °F
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic..
Mold Temperature 180 - 210 °C
356 - 410 °F
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c..
Mold Temperature 180 - 210 °C
356 - 410 °F
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced
General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex.
Mold Temperature 190 - 210 °C
374 - 410 °F
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
Mold Temperature 180 - 210 °C
356 - 410 °F
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant..
Mold Temperature 180 - 210 °C
356 - 410 °F
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac..
Mold Temperature 180 - 210 °C
356 - 410 °F
normal
Victrex® WG101™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai..
Mold Temperature 180 - 210 °C
356 - 410 °F
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS)  (Unverified Data**)
EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491°F), E..
Mold Temperature 190 - 210 °C
374 - 410 °F
Long flow or thin wall parts or for low residual stress
Solvay Specialty Polymers Supradel® HTS-2630 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2630 is a 30% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance ..
Mold Temperature 190 - 210 °C
374 - 410 °F
Long flow or thin wall parts or for low residual stress
Solvay Specialty Polymers Supradel® HTS-2420 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of 2..
Mold Temperature 190 - 210 °C
374 - 410 °F
Long flow or thin wall parts or for low residual stress
Solvay Specialty Polymers Supradel® HTS-2430 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of ..
Mold Temperature 190 - 210 °C
374 - 410 °F
Long flow or thin wall parts or for low residual stress
Solvay Specialty Polymers Supradel® HTS-2600 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2600 is a high-temperature, high-performance, amorphous, sulfone polymer. In addition to exceptional thermal performance, this resin has the other performance features and attributes t..
Mold Temperature 190 - 210 °C
374 - 410 °F
Long flow or thin wall parts or for low residual stress
Solvay Specialty Polymers Supradel® HTS-2601 High Temperature Sulfone Resin  (discontinued **)
Supradel HTS-2601 is a high-temperature high-performance amorphous sulfone polymer designed as a base resin for reinforced thermoplastic products. This exceptional thermal performance is available i..
Mold Temperature 175 - 210 °C
347 - 410 °F
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber
AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch..
Mold Temperature 180 - 210 °C
356 - 410 °F
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS)
EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491..
Mold Temperature 190 - 210 °C
374 - 410 °F
Long flow or thin wall parts or for low residual stress
Solvay Specialty Polymers Supradel® HTS-2620 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2620 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance ..
Mold Temperature 93.3 - 210 °C
200 - 410 °F
Average value: 146 °C Grade Count:11
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..
Mold Temperature 93.3 - 210 °C
200 - 410 °F
Average value: 153 °C Grade Count:8
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc..
Mold Temperature 180 - 210 °C
356 - 410 °F
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
Copyright © lookpolymers.com All Rights Reserved