Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cast Nylons Nycast® SLX Premium Bearing Grade Nylon

Category Polymer , Thermoplastic , Nylon
Manufacturer Cast Nylons Limited
Trade Name Nycast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cast Nylons Nycast® SLX Premium Bearing Grade Nylon.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nycast® SLX closes the gap between static and dynamic coefficients of friction. Used in wear pads, bearing blocks, and other load-bearing slide applications.Data provided by the manufacturer, Cast Nylons Limited.
Physical Properties Metric English Comments
Density 1.12 - 1.14 g/cc
0.0405 - 0.0412 lb/in³
ASTM D792
Water Absorption 0.032 %
0.032 %
24 hrs; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113 - 120
113 - 120
ASTM D785
Hardness, Shore D 75 - 84
75 - 84
ASTM D2240
Tensile Strength 69.6 - 70.3 MPa
10100 - 10200 psi
ASTM D638
Elongation at Break 38 - 47 %
38 - 47 %
ASTM D638
Tensile Modulus 3.17 GPa
460 ksi
ASTM D638
Flexural Strength 86.9 - 89.6 MPa
12600 - 13000 psi
ASTM D790
Flexural Modulus 2.51 - 2.59 GPa
364 - 376 ksi
ASTM D790
Compressive Strength 101 - 112 MPa
14600 - 16200 psi
ASTM D695
Compressive Modulus 1.87 - 1.97 GPa
271 - 286 ksi
ASTM D695
Shear Strength 58.9 - 59.2 MPa
8540 - 8590 psi
ASTM D732
Izod Impact, Notched 0.737 - 0.801 J/cm
1.38 - 1.50 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.14 - 0.19
0.14 - 0.19
ASTM D1894
Coefficient of Friction, Static 0.12 - 0.14
0.12 - 0.14
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear 74.5 - 75.1 µm/m-°C
41.4 - 41.7 µin/in-°F
Melting Point 221 °C
430 °F
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 - 72.2 °C
158 - 162 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved