Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 193 - 210 °C | 379 - 410 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging VB7 White 215 Polyvinyl Chloride, Rigid (PVC, Rigid) A rigid PVC Compound designed for extrusion blow molding balusters for railings.Information provided by PolyOne |
|||
Mold Temperature | 193 - 210 °C | 379 - 410 °F | Blow Molding |
PolyOne Geon™ Vinyl Packaging VEO-184 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Mold Temperature | 175 - 210 °C | 347 - 410 °F | |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic.. |
|||
Mold Temperature | 180 - 210 °C | 356 - 410 °F | |
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c.. |
|||
Mold Temperature | 180 - 210 °C | 356 - 410 °F | |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
Mold Temperature | 190 - 210 °C | 374 - 410 °F | |
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Mold Temperature | 180 - 210 °C | 356 - 410 °F | |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |
|||
Mold Temperature | 180 - 210 °C | 356 - 410 °F | |
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac.. |
|||
Mold Temperature | 180 - 210 °C | 356 - 410 °F | normal |
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |
|||
Mold Temperature | 180 - 210 °C | 356 - 410 °F | |
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS)
(Unverified Data**) EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491°F), E.. |
|||
Mold Temperature | 190 - 210 °C | 374 - 410 °F | Long flow or thin wall parts or for low residual stress |
Solvay Specialty Polymers Supradel® HTS-2630 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2630 is a 30% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance .. |
|||
Mold Temperature | 190 - 210 °C | 374 - 410 °F | Long flow or thin wall parts or for low residual stress |
Solvay Specialty Polymers Supradel® HTS-2420 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of 2.. |
|||
Mold Temperature | 190 - 210 °C | 374 - 410 °F | Long flow or thin wall parts or for low residual stress |
Solvay Specialty Polymers Supradel® HTS-2430 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of .. |
|||
Mold Temperature | 190 - 210 °C | 374 - 410 °F | Long flow or thin wall parts or for low residual stress |
Solvay Specialty Polymers Supradel® HTS-2600 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2600 is a high-temperature, high-performance, amorphous, sulfone polymer. In addition to exceptional thermal performance, this resin has the other performance features and attributes t.. |
|||
Mold Temperature | 190 - 210 °C | 374 - 410 °F | Long flow or thin wall parts or for low residual stress |
Solvay Specialty Polymers Supradel® HTS-2601 High Temperature Sulfone Resin
(discontinued **) Supradel HTS-2601 is a high-temperature high-performance amorphous sulfone polymer designed as a base resin for reinforced thermoplastic products. This exceptional thermal performance is available i.. |
|||
Mold Temperature | 175 - 210 °C | 347 - 410 °F | |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch.. |
|||
Mold Temperature | 180 - 210 °C | 356 - 410 °F | |
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS) EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491.. |
|||
Mold Temperature | 190 - 210 °C | 374 - 410 °F | Long flow or thin wall parts or for low residual stress |
Solvay Specialty Polymers Supradel® HTS-2620 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2620 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance .. |
|||
Mold Temperature | 93.3 - 210 °C | 200 - 410 °F | Average value: 146 °C Grade Count:11 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Mold Temperature | 93.3 - 210 °C | 200 - 410 °F | Average value: 153 °C Grade Count:8 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |
|||
Mold Temperature | 180 - 210 °C | 356 - 410 °F | |
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |