Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 200 MPa @Temperature 23.9 °C |
29000 psi @Temperature 75.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |
|||
Compressive Strength | 200 MPa @Temperature 120 °C |
29000 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c.. |
|||
Compressive Strength | 200 MPa @Temperature 120 °C |
29000 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
Compressive Strength | 200 MPa @Temperature 120 °C |
29000 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont.. |
|||
Compressive Strength | 200 MPa @Temperature 120 °C |
29000 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T.. |
|||
Compressive Strength | 200 MPa @Temperature 200 °C |
29000 psi @Temperature 392 °F |
|
Elisto THERMOSTAR® HD 800 Frame Press Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |
|||
Compressive Strength | 200 MPa @Temperature 23.0 °C |
29000 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F.. |