Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 65.0 MPa @Temperature 275 °C |
9430 psi @Temperature 527 °F |
ISO 178 |
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c.. |
|||
Flexural Strength | 65.0 MPa @Temperature 275 °C |
9430 psi @Temperature 527 °F |
ISO 178 |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
Flexural Strength | 65.0 MPa @Temperature 225 °C |
9430 psi @Temperature 437 °F |
ISO 178 |
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont.. |
|||
Flexural Strength | 65.0 MPa @Strain 8.00 % |
9430 psi @Strain 8.00 % |
cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS. |
|||
Flexural Strength | 65.0 MPa @Strain 8.00 % |
9430 psi @Strain 8.00 % |
Conditioned; ISO 178 |
Lanxess Durethan® BM 240 H3.0 000000 Nylon 6, 40% Mineral PA 6, 40% mineral, injection molding, heat-ageing stabilized, low tendency to warp, isotopic properties |
|||
Flexural Strength | 65.0 MPa @Temperature -40.0 °C |
9430 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 2.0%); ASTM-D790 |
Toyobo GLAMIDE® T-777-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 65.0 MPa @Thickness >=1.50 mm |
9430 psi @Thickness >=0.0591 in |
1hr/130°C/measured at 130°C; ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m.. |
|||
Flexural Strength | 65.0 MPa @Thickness >=1.50 mm |
9430 psi @Thickness >=0.0591 in |
1hr/130°C/measured at 130°C; ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax PM GPO 3 Polyester, Glass Mat, Red, Sheets Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free.Applica.. |