| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
| Water Absorption | 7.0 % | 7.0 % | ISO 62 |
| Moisture Absorption | 2.00 % | 2.00 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4, 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Ball Indentation Hardness | 85.0 MPa | 12300 psi | conditioned; ISO 2039-1 |
| 170 MPa | 24700 psi | dry; ISO 2039-1 | |
| Tensile Strength at Break | 105 MPa | 15200 psi | conditioned; ISO 527-1/-2 |
| 150 MPa | 21800 psi | dry; ISO 527-1/-2 | |
| Elongation at Break | 4.0 % | 4.0 % | dry; ISO 527-1/-2 |
| 8.0 % | 8.0 % | conditioned; ISO 527-1/-2 | |
| Tensile Modulus | 5.50 GPa | 798 ksi | conditioned; ISO 527-1/-2 |
| 8.50 GPa | 1230 ksi | dry; ISO 527-1/-2 | |
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | dry; ISO 179/1eU |
| 9.50 J/cm² | 45.2 ft-lb/in² | conditioned; ISO 179/1eU | |
| 8.00 J/cm² <br>@Temperature 30.0 °C |
38.1 ft-lb/in² <br>@Temperature 86.0 °F |
dry; ISO 179/1eU | |
| 8.50 J/cm² <br>@Temperature 30.0 °C |
40.4 ft-lb/in² <br>@Temperature 86.0 °F |
conditioned; ISO 179/1eU | |
| Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | dry; ISO 179/1eA |
| 2.50 J/cm² | 11.9 ft-lb/in² | conditioned; ISO 179/1eA | |
| 1.10 J/cm² <br>@Temperature 30.0 °C |
5.23 ft-lb/in² <br>@Temperature 86.0 °F |
dry; ISO 179/1eU | |
| 1.20 J/cm² <br>@Temperature 30.0 °C |
5.71 ft-lb/in² <br>@Temperature 86.0 °F |
conditioned; ISO 179/1eU |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
| 180 °C | 356 °F | short term; EMS | |
| Deflection Temperature at 1.8 MPa (264 psi) | 200 °C | 392 °F | ISO 75-1/-2 |
| Deflection Temperature at 8.0 MPa | 85.0 °C | 185 °F | ISO 75-1/-2 |
| Flammability, UL94 | HB | HB | IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | conditioned; IEC 60093 |
| 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | dry; IEC 60093 | |
| Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
| 41.0 kV/mm | 1040 kV/in | dry; IEC 60243-1 | |
| Comparative Tracking Index | 550 V | 550 V | conditioned; IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Form | Granules | |
| Processing | Injection Molding | |
| Special Characteristics | High impact or impact modified |