Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 9.50 J/cm² @Temperature -30.0 °C |
45.2 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® 513RS PC (Europe-Africa-Middle East) LEXAN 513RS is a medium viscosity, glass reinforced, flame retardant grade UV stabilized grade. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
Radici Radilon® ARV300 RKC (dry) Nylon 66 Glass-fiber reinforced with heat and hydrolysis resistanceInformation provided by Radici group. |
|||
Charpy Impact Unnotched | 9.50 J/cm² - NB | 45.2 ft-lb/in² - NB | Average value: 9.50 J/cm² Grade Count:11 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² - NB @Temperature -30.0 - -30.0 °C |
45.2 ft-lb/in² - NB @Temperature -22.0 - -22.0 °F |
Average value: 9.50 J/cm² Grade Count:10 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1-7830 Polyamide 66, with PTFE, lubricant modified, improved wear resistance, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/EU-1993 |
Solvay Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH50 Polyamide PA66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V30 is used in all sectors of industry, offering an excellent combination between thermal and.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218G V30 PA66, 30% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding specially stabilized to improve its resistance automotive cooling liquids.Available in: Europe and Latin Americ.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, Conditioned Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, heat and UV stabilized, characterized by a high fluidity of the melt, for injection molding.Available in: Europe Product Applic.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature -30.0 °C |
45.2 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Xenoy® X2420 PC+POLYESTER (Asia Pacific) Xenoy*X2420 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and impact strength. X2420 has enhanced melt flowability, impact ductility and broad co.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 216 V30 PA66, 33% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: TECHNYL A 216 V30 is .. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP STAT-KON DX02437 PC (Asia Pacific) LNP Stat-Kon DX02437 is a compound based on Polycarbonate resin containing conductive carbon powder, with good impact-resistance, flow and ESD performance, suitable for semi-con industry. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® 2SV-30H black 9992 PA610-GF30 Product Description: GRILAMID XE 3976 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® B 70 GFE 30 H PA6-GF30 Product description: Grilon B 70 GFE 30 H is a heat stabilized and impact modified PA 6 injection molding grade with 30% glass fiber reinforcement. Grilon B 70 GFE 30 H has the following important p.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® BGZ-50/2 PA6-I-GF50 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW200F8 (COND) Nylon 46 40% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-50/4 black 9833 PA666-GF50 Product description: Grilon TSGL-50/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 black is characterized by the following key-p.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 30.0 °C |
45.2 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-50-4 black 9839 PA666-GF50 Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following .. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 30.0 °C |
45.2 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-60/4 black 9833 PA666-GF60 Product description: Grilon TSGL-60/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black is characterized by the following key-p.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 30.0 °C |
45.2 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4105 nat PA610-GF50 Product description: Grilamid XE 4105 natural is a 50% glass fiber reinforced, heat stabilized polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 30.0 °C |
45.2 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4106 black 9992 PA612-GF30 Product description: Grilamid XE 4106 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorpti.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK416 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 resin for injection molding.Information provided by.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T BK261 is a 30% glass fiber reinforced toughened black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Conditioned, 60% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179 1eU |
Azoty Tarnow™ Tarnamid® T-27 GF35 Polyamide 6 - Glass Fiber Reinforced 35% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4192 black 9992 PA610-GF30 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 30.0 °C |
45.2 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® LBV-50H FWA black 9225 PA12-GF50 Product Description: Grilamid LBV-50H FWA black 9225 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® LBV-50H FWA nat PA12-GF50 Product Description: Grilamid LBV-50H FWA natural is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |