Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 180 °C | 356 °F | UL Temperature Index per UL746B |
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® BR42B is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surf.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
Lehmann & Voss LUVOCOM® 1301-7953 PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | short term |
Lehmann & Voss LUVOCOM® 1502-7866/GN4 PPSU, unreinforced Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
Freudenberg Simrit F80 Fluorosilicone Elastomer Combines excellent low-temperature performance of silicone with improved chemical resistance. Very good resistance to military and aerospace fuels. Excellent performance in oxygen plasma environment.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
GEHR Plastics PPSU Polyphenylenesulfone Polyphenylenesulfone is an amorphous material, with improved impact and hydrolysis resistance compared to PSU. The usual operating temperature is approximately 180°C. The extremely high notched i.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | short term |
Lehmann & Voss LUVOCOM® 1800-7519 PET, with carbon fiber, PTFE, mineral resin Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous d.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
Lehmann & Voss LUVOCOM® 1100-8134 Polyether sulfone, with carbon fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
Silikony Polskie Gumosil B Silicone Rubber Flexible with low hardness |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2514S-40-10 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2521S-10-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 25235-60-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | UL Temperature Index; UL 746B |
Sumitomo Bakelite North America RX® 611 Fiberglass Reinforced Phenolic RX 611 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type MFH.Information supplied by Sumitomo.. |
|||
Maximum Service Temperature, Air | >= 180 °C | >= 356 °F | Short peaks operation |
Polyram PA500 Nylon 6.6, Flame Retardant Flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
Von Roll Isola IMI Varnish 701 Solventless Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: 42°C. Usag.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | Short peaks operation |
Polyram PlusTek PA804 Nylon 6.6 for Injection Molding, Impact Modified Impact modified Nylon 6.6 for injection molding application.Information provided by Polyram. |
|||
Maximum Service Temperature, Air | >= 180 °C | >= 356 °F | Short peaks operation |
Polyram PlusTek PA841 Nylon 6.6, Impact Modified Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | Short peaks operation |
Polyram PlusTek PB150 Nylon 6, Injection Molding Fast cycle polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | >= 180 °C | >= 356 °F | Short peaks operation |
Polyram PlusTek RA845 Nylon 6.6, Impact Modified Improved impact polyamide 6.6 for good resistance to low temp for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | Continuous Use |
Westlake Plastics PES film Made from ULTRASON® E Polyethersulfone Resin High heat deflection and continuous use temperature. Exceptional tensile and flexural strength. High dielectric strength. Exceptional mechanical properties. Dimensionally stable at varying tempera.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | short term; EMS |
EMS-Grivory Grivory® BGZ-50/2 PA6-I-GF50 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | short term; EMS |
EMS-Grivory Grivory® BS PA6 Product description: Grilon BS is an unreinforced, heat stabilized standard PA6 injection molding grade with normal melt viscosity. Grilon BS has the following important properties: Good flow behavi.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | short term; EMS |
EMS-Grivory Grivory® BS/2 PA6 Product description: Grilon BS/2 is an unreinforced, nucleated standard PA6 injection molding grade with normal melt viscosity. Grilon BS/2 has the following important properties: Good flow behavior.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | short term; EMS |
EMS-Grivory Grivory® ELX 40 HNZ TPA Product description: Grilon ELX 40 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow moulding applications. Grilon ELX 40 H NZ has the follow.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | short term; EMS |
EMS-Grivory Grivory® TSGK-30 X PA666-(GF+GB)30 Product description: Grilon TSGK-30 X is a heat stabilized PA66 + PA6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30 X has the following .. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | Continuous |
Epoxy Technology EPO-TEK® H35-175MPLV Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H35-175MPLV is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-el.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Conditioned) Description: 20% mineral-filled and 10% glass-fiber reinforced injection-molding grade with outstanding flowability for technical parts with medium rigidity and high dimensional stability, e.g. for.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | short cycle operations |
BASF Ultrason S 2010 G4 20% Glass Filled PSU Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | Short term |
CENTROPLAST CENTRO HPM Polysulfone This plastic has good hydrolysis, chemical and radiation resistance, and can operate at high temperatures. It is used in food processing industry, pumps and valves, and medical equipment.Informatio.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | Two Hour Heat Resistance per ASTM D648 |
Chang Chun Plastic Longlite PM T308J General Purpose Phenolic Molding Compound ASTM Grade per ASTM D700 is 3.Information provided by Dowell Trading Company Ltd. |