Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Polimeri Europa Sinkral® B 432/E ABS Resin
Sinkral B 432/E is a general purpose extrusion grade which exhibits a good balance between rigidity and toughness. Designation: Thermoplastic ISO 2580-ABS 1,EGN,105-04-16-20Applications: Large sheet..
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO.179 DN.53453
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300
PE 300: Polyethylene with high density. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monom..
Charpy Impact, Notched 1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYabs S20 ABS
Information provided by Polykemi AB
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics Lexan® BFL2015 PC
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® FXE121R PC (Europe-Africa-Middle East)
LEXAN FXE121R is a transparent/translucent low viscosity grade for special effects colors with a fluorescent appearance. Color package may affect performance.
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® HF1130R PC (Europe-Africa-Middle East)
LEXAN HF1130R is a high flow, UV stabilized, grade especially designed for applications that require thin wall sections and higher flow lengths.
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® HP1R PC (Asia Pacific)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount..
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® LUX2114G PC (Asia Pacific)
18 MFR. Improved flame retardance. Internal mold release. UV stabilized.
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® BFL2000 PC (Europe-Africa-Middle East)
Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors.
Charpy Impact, Notched 1.20 - 1.60 J/cm²

@Thickness 3.00 - 3.00 mm
5.71 - 7.61 ft-lb/in²

@Thickness 0.118 - 0.118 in
Average value: 1.62 J/cm² Grade Count:4
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Charpy Impact, Notched 1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Grupo Repol Dinalon® A1S25 G30XV0 PA66 30% Glass Fiber V0
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® A 218G V33 Black 34N PA66, 25% glass fiber, DRY
Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail..
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, DRY
Description: TECHNYL® A 216 V33 is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This product is available in natural color.Benefits: The product offers an excellent ..
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179
Styrolution Terblend® N NG-02 8% Glass Filled ABS/PA6 (Dry)
Terblend N NG-02 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, high impact strength and good surface appearance.Information provided by STYROLUTION, which is a join..
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
IS0179-1:2000
Zhejiang Juner JEPP2007 PP For Automotive Parts
Applications: Inner Decorate PartsInformation provided by Zhejiang Juner New Materials Co, Ltd.
Charpy Impact, Notched 1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® BG-60 FC PA6-GF60
Product description: Grilon BG-60 FC is a heat stabilized PA6 injection molding grade with 60% glass fibers. Grilon BG-60 FC has the following important properties: Short cycle timesExcellent surfac..
Charpy Impact, Notched 1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® BGZ-50/2 PA6-I-GF50
Information provided by EMS Grivory
Charpy Impact, Notched 1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® BT 40 Z PA6
Product description: Grilon BT 40 Z is an unreinforced, normal viscosity, impact modified polyamide blend with amorphous and semi-crystalline components. Grilon BT 40 Z has the following important p..
Charpy Impact, Notched 1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600 GS 15 HWCP 15% Glass Sphere Filled Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact, Notched 1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® TSG-50/4 PA666-GF50
Product description: Grilon TSG-50/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50/4 has the following important properties: High sti..
Charpy Impact, Notched 1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® TSGZ-50 PA666-GF50
Information provided by EMS Grivory
Charpy Impact, Notched 1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® XE 3997 nat PAMACM12
Product description: Grilamid XE 3997 natural is a transparent thermoplastic polyamide based on aliphatic and cycloaliphatic blocks. Grilamid XE 3997 natural is particularly suitable for blow molded..
Charpy Impact, Notched 1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® XE 4065 black 9238 PA*-GF50
Product description: Grivory XE 4065 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia..
Charpy Impact, Notched 1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® XE 4104 nat PA610-GF40
Product description: Grilamid XE 4104 natural is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw materia..
Charpy Impact, Notched 1.20 J/cm²

@Temperature -40.0 °C
5.71 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612
33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
dry; ISO 179/1eA
EMS-Grivory Grivory® HT1V-65H black 9205 PA6T/6I-GF65
Product description: Grivory HT1V-65H black 9205 is a 65% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I..
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
conditioned; ISO 179/1eA
EMS-Grivory Grivory® HT1V-65H black 9205 PA6T/6I-GF65
Product description: Grivory HT1V-65H black 9205 is a 65% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I..
Charpy Impact, Notched 1.20 J/cm²

@Temperature -20.0 °C
5.71 ft-lb/in²

@Temperature -4.00 °F
Dry; ISO 179/Af
Arkema Group Orgalloy® RS 6000 Polyamide 6 Alloy
Polyamide Alloy, Rigid grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Asia Pacific)
Improved flow PC with excellent processability and mold release.
Charpy Impact, Notched 1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® BGZ-15/2 PA6-GF15
Product description: Grilon BGZ-15/2 is a heat stabilized and impact modified PA6 injection molding grade with 15% glass fibers. Grilon BGZ-15/2 has the following important properties: Good impact s..
Copyright © lookpolymers.com All Rights Reserved