Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.45 GPa | 1230 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ NL-30GF/15T Black Polyamide 612 (Nylon 612) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-2 |
PolyOne Nymax™ GMF 604 40 UV Black 28 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Tensile Modulus | 8.50 GPa @Temperature 23.0 °C |
1230 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ A70 G25 H U-SO Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-2 |
PolyOne Nymax™ X GMF 604 40 UV Black 148 rev 4 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | 1 mm/min; ISO 527 - 1/2 |
Hexion Bakelite™ PF 2535 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof
(discontinued ** Phenolic molding compound, inorganically/organically filled, average heat resistant, steam resistant, dish washer proof, high surface quality.Application areas: Fittings for ovens and dishwashers, t.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1/-2 |
Lanxess Pocan® BF 4225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, flame retardant |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | |
LATI Laticonther 62 CPG/500 PA 6, Glass Fiber Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218G V33 Black 41N PA66, 33% glass fiber, DRY Description: TECHNYL® A 218G V33 Black 41N is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This pr.. |
|||
Tensile Modulus | 8.46 GPa | 1230 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP WFL34H PBT LNP LUBRICOMP* WFL34H is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Healthcare. |
|||
Tensile Modulus | 8.46 GPa | 1230 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66 LNP LUBRILOY* RF206 is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant, Added features of this material includes: Wear Resistant. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP ZF006 PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF006 is a compound based on PPE+PS Blend resin containing Glass Fiber |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon DE002P PC (Asia Pacific) LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
Tensile Modulus | 8.48 GPa | 1230 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon DX96690 PC LNP STAT-KON* DX96690 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the America.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | 1mm/min; ISO 527 |
Teijin Panlite® GV-3430R High Flame Retardancy, Glass Fiber Reinforced Polycarbonate Resin GF 30% reinforced, improved flame retardance and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecis.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ASTM D638 |
Plenco 2308 Phenolic, Granular, Compression Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ASTM D638 |
Plenco 3509 Phenolic, Granular, Injection Molded PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ASTM D638 |
Plenco 4485 Phenolic, Granular, Compression Molded PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a.. |
|||
Tensile Modulus | 8.50 - 10.0 GPa | 1230 - 1450 ksi | ISO 527 |
Vyncolit 4451 XB Novolac Phenolic Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1/-2 |
DSM Akulon® K224-PG6 Impact Modified Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1/-2 |
DSM Arnite® TV4 241 SN PBT-GF20 FR(17) 20% Glass Reinforced, Flame Retardant |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-25 S PA6-GF25 Product description: Grilon BG-25 S is a heat stabilized PA6 injection molding grade with 25 % glass fibers. Grilon BG-25 S has the following important properties: Excellent surface finishEasy flowi.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-40 HM PA6-GF40 Product description: Grilon BG-40 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 40% glass fibers. Grilon BG-40 HM has the following important prop.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 GV 30 HW 30% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 GV 35 HWCP 35% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGK-30 X PA666-(GF+GB)30 Product description: Grilon TSGK-30 X is a heat stabilized PA66 + PA6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30 X has the following .. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® HR5330HF BK503 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide PF006ES PA6, 30% Glass Fiber Filled, Injection Molded Staramide PF006ES is a 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527 |
Eurotec® Tecomid® NA40 GR25 NL HS PA6.6, 25% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 8.48 GPa | 1230 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON QE002S PA6.10 LNP* STAT-KON* QE002S is a compound based on Nylon 6/10 containing 10% carbon Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive. |