Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.50 J/cm² | 40.5 ft-lb/in² | |
Polimeri Europa EDISTIR PD RK4122H High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,078-06-04-23 UL94 V-2, halogen and antimony free, medium impact polystyrene. This grade features enhanced thermal stabi.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² - NB | 40.5 ft-lb/in² - NB | Average value: 9.25 J/cm² Grade Count:25 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² - NB @Temperature -30.0 - -30.0 °C |
40.5 ft-lb/in² - NB @Temperature -22.0 - -22.0 °F |
Average value: 10.1 J/cm² Grade Count:23 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® DP 2004 000000 PBT PBT, non-reinforced, injection molding, halogen free flame retardant |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | |
LATI Laramid G/45 PPA, 45% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | |
LATI Latamid 6 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | |
LATI Latigloss 66 H2 G/50 F2 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Potentially suitable for food/medical contact application. Availab.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.5 ft-lb/in² | Conditioned; ISO 179/1eU |
Solvay Technyl® A 60G1 V25 25% Glass Reinforced Nylon 66, Flame Retardant This Red Phosphorous and Halogen free flame retardant grade, combines excellent all-round mechanical properties with outstanding flame retardancy (UL 5VA at 1.6mm) and electrical performance. This p.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® C 218 MZ20 V10 Black Z PA6, 20/10% mineral/glass fiber, Conditioned Description: Polyamide PA6, reinforced 20 % mineral filler and 10 % of glass fiber, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL C 218 MZ20 V10 offe.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® 1SVX-50H nat PA1010-GF50 Product Description: Grilamid 1SVX-50H natural is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® 1SVX-65H black 9288 PA1010-GF65 Product Description: Grilamid 1SVX-65H black is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources Exc.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BG-15 PA6-GF15 Product description: Grilon BG-15 is a heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon BG-15 has the following important properties: Good surface finishGood b.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BM-30 FR PA6-MD30 FR Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GVN-35H black 9915 PA*-GF35 Product description: Grivory GVN-35H is a 35% glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600/58 GV 30 HWCP 30% Glass Fiber Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LVX-50H nat PA12-GF50 Product description: Grilamid LVX-50H natural is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are: Very high stiffness and st.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSC-30/4 EC black 9832 PA666-CF30 Product description: Grilon TSC-30/4 EC is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers. Grilon TSC-30/4 EC has the following important properties:El.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-30 PA666-GF30 Product description: Grilon TSG-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30 has the following important properties: Excellent fl.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® TSG-35 PA666-GF35 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-35/4 PA666-GF35 Product description: Grilon TSG-35/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers. Grilon TSG-35/4 has the following important properties: Good flo.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4104 black 9992 PA610-GF40 Product description: Grilamid XE 4104 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4107 nat PA612-GF40 Product description: Grilamid XE 4107 natural is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorptiong.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-50 S PA6-GF50 Product description: Grilon BG-50 S is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 S has the following important properties: High stiffnessExcellent surface fin.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GVL-6H black 9915 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | cond.; ISO 179 1eU |
Azoty Tarnow™ Tarnamid® T-27 GF15 I Polyamide 6 - Glass Fiber Reinforced 15% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry) Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.5 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® MN301-G30 Nylon 66 Resin 30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |