Polymer Property : Linear Mold Shrinkage, Transverse = 0.0060 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ISO 294-4
Polyplastic Armamid® PA GF50-1 Nylon 6, 50% Glass Fiber
High stiffnessInformation provided by PolyPlastic Group.
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0060 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER
Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm ..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0060 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Asia Pacific)
Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0060 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® ML7682 PC Copolymer (Asia Pacific)
Lexan ML7682 resin is a flame retardant polycarbonate blend featuring high flow, good processability, good impact, good heat resistance, and UV stability. It is of non-chlorine and non-bromine flame..
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ISO Data (Dry)
BASF Capron® GR40 HS 40% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron GR40 HS is a heat stabilized 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stabil..
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
Euronil
Nilit Nilamid B G6 FR HF 30% Glass Fiber Reinforced, Flame Retardant PA6
Description: Nilamid B G6 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price..
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
Euronil
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid..
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
380°C nozzle, 190°C tool; ISO 294-4
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac..
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ASTM D955
LNP Thermocomp® GF-1006 Polysulfone, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
Chevron Phillips Xtel® XK2760BL Polyphenylene Sulfide Alloy  (discontinued **)
Xtel® XK2760BL is a high performance, glass fiber and mineral filled PPS based alloy developed to provide excellent mechanical strength with a unique blend of toughness, rigidity, and low flash cha..
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
Test Condition: 60x60x2; 260°C / MT 80°C; 500 bar; ISO 294-4
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (Conditioned), Injection Molding Grade
Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage.
Linear Mold Shrinkage, Transverse 0.0060 cm/cm

@Temperature 80.0 °C
0.0060 in/in

@Temperature 176 °F
60x60x2 mm; ISO 294-4
Gromax BFG45-DN00N1 Nylon 6 46% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Linear Mold Shrinkage, Transverse 0.0060 - 0.0090 cm/cm
0.0060 - 0.0090 in/in
LATI Laramid G/45 PPA, 45% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Linear Mold Shrinkage, Transverse 0.0060 cm/cm

@Temperature 80.0 °C
0.0060 in/in

@Temperature 176 °F
60x60x2 mm; ISO 294-4
Gromax BFG30-EN03N1 Nylon 6 33% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
LATI Latamid 68 H2-V0 PA6/PA66 copolymer, Heat Stabilized, Flame Retardant
PA6/PA66 copolymer (PA6/PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Good surface appearance.Availability: Africa & Middle Ea..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0090 cm/cm
0.0060 - 0.0090 in/in
LATI Latiohm 62-09 PD01 G/20-V2HF PA6, 20% Glass Fiber Reinforced, Flame Retardant
Semiconductive/dissipative product based on Polyamide 6 (PA6). Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Very good mechanical properties.Availabili..
Linear Mold Shrinkage, Transverse 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
on tensile bar; SABIC Method
SABIC Innovative Plastics Valox® VX8015U PBT+PET (Europe-Africa-Middle East)
VALOX VX8015U is a UV stabilized, 15% glass reinforced PBT+PET injection moulding resin with improved surface finish quality characteristics versus VALOX 815. This grade is 815 with improved gloss a..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm

@Time 86400 sec
0.0060 - 0.0080 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP DF002 PC
LNP THERMOCOMP* DF002 is a compound based on Polycarbonate resin containing 10% Glass Fiber.
Linear Mold Shrinkage, Transverse 0.0060 cm/cm

@Thickness 3.20 mm
0.0060 in/in

@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Starex® MG-0330 ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Linear Mold Shrinkage, Transverse 0.0060 - 0.0090 cm/cm
0.0060 - 0.0090 in/in
SABIC Method
SABIC Innovative Plastics Valox® SHF4930 PBT
Super high flow FR PBT grade with 15% Glass reinforced
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® BG-30 S FA PA6-GF30
Product description: Grilon BG-30 S FA is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S FA has the following important properties: Excellent surface finishEasy ..
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6  (Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performan..
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® FR95G25V0NH NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 ZYTEL FR95G25V0NH NC010 is 25% glass fiber reinforced flame retardant polyamide halogen and red phosphorous free with high flow and excellent long t..
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® PLS 95G50DH2 BK261 Nylon 6  (Unverified Data**)
50% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology only from DuPont providing exceptional Heat Resistanc..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
E-Polymers TEKAMID® JN930 PPE+PA66 30% Glass Fiber Reinforced PA/PPE Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ISO 294-4
Celanese Celanex® 7714 PBT, Mineral / Glass Reinforced
Celanex 7714 is a 35% glass/mineral reinforced, non-exuding, flame retartant PBT which has an excellent balance of mechanical properties and processability. Celanex 7714 is well suited for electric..
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ISO 294-4
Celanese Celanex® 3325HRT PBT, 30% Glass Reinforced
Celanex 3325HRT is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate copolymer that has excellent hydrolysis resistance, toughness, improved flow, and improved elongation at bre..
Linear Mold Shrinkage, Transverse 0.0060 cm/cm

@Thickness 2.00 mm
0.0060 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66  (Unverified Data**)
Zytel® 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was developed for applications requiring strength, stiffness and im..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0060 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER (Asia Pacific)
Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U..
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ASTM D955
Lubrizol Estane® 2103-90AENH Film Grade Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: NSF Standard 61 Certified, FDA ComplianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane prod..