Polymer Property : Dielectric Strength = 41.0 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 41.0 kV/mm

@Thickness 0.800 mm
1040 kV/in

@Thickness 0.0315 in
Short Term; ASTM D149
Shell Carilon® DB6F5G40 Polyketone, Flame-Retarded (V-0), 20% Glass-Reinforced Injection Molding Grade  (disco
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6F5G40 is a flame-retarded, 20 percent glass-fiber-reinforced, injection molding grade with mecha..
Dielectric Strength 41.0 kV/mm

@Thickness 0.800 mm
1040 kV/in

@Thickness 0.0315 in
Short Term; ASTM D149
Shell Carilon® DB6F1G30 Polyketone, Flame-Retarded, Tracking-Resistant, Glass-Reinforced Injection Molding Grade &n
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6F1G30 is a flame-retarded, 15 percent glass-fiber-reinforced, injection molding grade with mecha..
Dielectric Strength 41.0 kV/mm
1040 kV/in
IEC 60243
Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, DRY
Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This gr..
Dielectric Strength 41.0 kV/mm

@Thickness 1.50 mm
1040 kV/in

@Thickness 0.0591 in
Short Time; IEC 60243-1
Styrolution Novodur® HH-112 ABS
Novodur HH-112 is a high heat injection molding grade. It provides good heat resistance combined with enhanced stiffness.Information provided by Styrolution
Dielectric Strength 41.0 kV/mm
1040 kV/in
IEC 60243-1
Styrolution Terblend® N NM-11 ABS/PA6 (Dry)
Terblend N NM-11 is an ABS/PA6 blend combining very high impact strength, even at low temperatures, with an excellent processability and surface appearance.Information provided by STYROLUTION, which..
Dielectric Strength 41.0 kV/mm
1040 kV/in
IEC 60243-1
Styrolution Terblend® N NM-12 ABS/PA6 (Dry)
Terblend N NM-12 is an ABS/PA6 blend combining high impact strength and rigidity with an excellent processability and surface appearance.Information provided by STYROLUTION, which is a joint venture..
Dielectric Strength 41.0 kV/mm
1040 kV/in
IEC 60243-1
Styrolution Terblend® N NM-19 ABS/PA6 (Dry)
Terblend N NM-19 is a UV stabilized ABS/PA6 blend combining very high impact strength, even at low temperatures with an excellent processability and surface appearance.Information provided by STYROL..
Dielectric Strength 41.0 kV/mm
1040 kV/in
IEC 60243-1
Styrolution Terblend® N NMX04 ABS/PA6 (Dry)
Terblend N NMX04 is an ABS/PA6 blend specially developed for painted exterior applications, combining impact resistance with excellent processability and paintability.Information provided by STYROLU..
Dielectric Strength 41.0 kV/mm
1040 kV/in
IEC 60243-1
Styrolution Terluran® HH-112 ABS
Terluran HH-112 is an injection molding grade of ABS with very high heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Dielectric Strength 41.0 kV/mm
1040 kV/in
K20/P50; IEC 60243-1
Styrolution Terluran® HH-112 Q109 ABS
Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Dielectric Strength 41.0 kV/mm
1040 kV/in
K20/P50; IEC 60243-1
Styrolution Terluran® HH-112 Q42 Gray 10072 ABS
Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Dielectric Strength 41.0 kV/mm
1040 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® AG-35 PA66-GF35
Product description: Grilon AG-35 is a heat stabilized, normal viscosity PA 66 injection molding grade with 35% glass fibers. High stiffnessHigh tensile strengthHigh heat distortion temperatureEasy ..
Dielectric Strength 41.0 kV/mm
1040 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® BG-40 HM PA6-GF40
Product description: Grilon BG-40 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 40% glass fibers. Grilon BG-40 HM has the following important prop..
Dielectric Strength 41.0 kV/mm
1040 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® BGZ-30/2 PA6-GF30
Product description: Grilon BGZ-30/2 is a heat stabilized and impact modified PA6 injection molding grade with 30% glass fibers. Grilon BGZ-30/2 has the following important properties: Good impact s..
Dielectric Strength 41.0 kV/mm
1040 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® BGZ-50/2 PA6-I-GF50
Information provided by EMS Grivory
Dielectric Strength 41.0 kV/mm
1040 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® XE 4105 nat PA610-GF50
Product description: Grilamid XE 4105 natural is a 50% glass fiber reinforced, heat stabilized polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw..
Dielectric Strength 41.0 kV/mm
1040 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® BGZ-40 PA6-GF40
Product description: Grilon BGZ-40 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 40% glass fibers. Grilon BGZ-40 has the following important properties:..
Dielectric Strength 41.0 kV/mm
1040 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® XE 5051 (BGZ-40 FC) PA6-GF40
Product description: Grilon XE 5051 is a impact modified, heat stabilized PA 6 injection molding grade with 40% glass fiber reinforcement. Grilon XE 5051 has the following important properties: High..
Dielectric Strength 41.0 kV/mm
1040 kV/in
IEC 243/1
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT
Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 30% of glass fibers for industrial parts with high dimensional stab..