Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 9.50 J/cm² - NB | 45.2 ft-lb/in² - NB | Average value: 9.50 J/cm² Grade Count:11 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² - NB @Temperature -30.0 - -30.0 °C |
45.2 ft-lb/in² - NB @Temperature -22.0 - -22.0 °F |
Average value: 9.50 J/cm² Grade Count:10 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1106-8032/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature -30.0 °C |
45.2 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® 488 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1/XCF/30 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1100-7939/GY Polyether sulfone, unreinforced Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1106-8232 Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1-3260/schwarz Polyamide 66, with PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOTECH® GS 58 Polyamide 66, with glass fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218 V43 Black 21 N PA66, 43% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 43% of glass fiber, heat stabilized, for injection molding.Available in: North AmericaProduct Applications: TECHNYL® A 218 V43 is used in all sectors .. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, Conditioned Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, Conditioned Description: TECHNYL STAR TM Polyamide reinforced with 60% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North America Product Applicat.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYLSTARâ„¢ SX 218 V60 Black Z PA6, 60% glass filled, Conditioned Description: TECHNYLSTAR Polyamide reinforced with 60% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Asia Pacific, Europe and No.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature -30.0 °C |
45.2 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Xenoy® X2420 PC+POLYESTER (Asia Pacific) Xenoy*X2420 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and impact strength. X2420 has enhanced melt flowability, impact ductility and broad co.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30 Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30 Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® AG-30 PA66-GF30 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GV 15 HWCP 15% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GVS 20/10 HWCP 20% Glass Fiber and 10% Glass Sphere Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 30.0 °C |
45.2 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GVL-6H nat PA*-GF60 Product description: Grivory GVL-6H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H na.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 30.0 °C |
45.2 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-50-4 black 9839 PA666-GF50 Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following .. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4104 nat PA610-GF40 Product description: Grilamid XE 4104 natural is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw materia.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 30.0 °C |
45.2 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4106 black 9992 PA612-GF30 Product description: Grilamid XE 4106 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorpti.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T BK261 is a 30% glass fiber reinforced toughened black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4192 black 9992 PA610-GF30 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® LBV-50H FWA nat PA12-GF50 Product Description: Grilamid LBV-50H FWA natural is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 30.0 °C |
45.2 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® LBV-50H FWA nat PA12-GF50 Product Description: Grilamid LBV-50H FWA natural is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |