Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218 V25 Black 21NHFE PA66, 25% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218 V25 NAT BA PA66, 25% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218 V25 Natural B PA66, 25% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218 V30 Black 21 NHFE PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH0 |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH50 |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218G V30 PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218G V30 PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218G V33 Black 34N PA66, 25% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218G V33 Black 34N PA66, 25% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218G1 V30 Black 34N PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218G1 V30 Black 34N PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218W V30 Black FA PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 21T2 V25 PA66, 25% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 21T2 V25 PA66, 25% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 60 G1 V30 PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 60 G1 V30 PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 60 G2 V30 PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 60 G2 V30 PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 718 V30 PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay Technyl® A218GV33-BK 33% Glass Filled, Heat Stabilized, Hydrolysis Resistant, Black Nylon 66 |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® B 218L V20 Black 44 N PA66, 25% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® B 218L V20 Black 44 N PA66, 25% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® R AR 130/GF Nylon 66, 30% glass fiber, Conditioned |
Renewable/Recycled Polymer |
TECHNYL® R
|
Solvay TECHNYL® R AR 130/GF Nylon 66, 30% glass fiber, DRY |
Renewable/Recycled Polymer |
TECHNYL® R
|
Solvay TECHNYL® R AR 218 V30 Nylon 66, 30% glass fiber, DRY |
Renewable/Recycled Polymer |
TECHNYL® R
|
Solvay TECHNYL® A 216 S30 PA66, 30% glass spheres, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218 PA66, 33% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218 V30 Black 21 NHFE PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218W V30 Black FA PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® AR 218 V25 Nylon 66, 25% glass fiber, DRY |
Renewable/Recycled Polymer |
Technyl®
|
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 216 V30 Natural FA PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0 |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH50 |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® 2411GF6 PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® 2411GF6 PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 216 V30 Natural FA PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218 S30 Black 21 N PA66, 30% glass fiber, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218 S30 Black 21 N PA66, 30% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY |
Nylon 66, 30% Glass Fiber Filled |
Technyl®
|