Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding. This product is available in Natural & Black. Key Properties: UL94 V0 at 0.8mm and Excellent filling qualitiesBenefits: This Red Phosphorous flame retardent grade provides robust UL 94 V-0 and a full UL yellow card while offering good mechanical properties. This grade is suitable for moulding insulating parts for electrical devices, and more generally for thin parts under stress. Available in: Asia Pacific, Europe, Latin America and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/E.C.This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applicationsApplications: Industrial controls and electrical insulation systemInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 105 MPa
15200 psi
ISO 527 Type 1A
Elongation at Break 4.1 %
4.1 %
ISO 527 Type 1A
Tensile Modulus 6.50 GPa
943 ksi
ISO 527 Type 1A
Flexural Strength 155 MPa
22500 psi
ISO 178
Flexural Modulus 6.00 GPa
870 ksi
ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 25.0 kV/mm
635 kV/in
IEC 60243
Dissipation Factor 0.050
0.050
IEC 60250
Comparative Tracking Index 350 V
350 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %