Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 218W V30 Black FA PA66, 30% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218W V30 Black FA PA66, 30% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance.Available in: EuropeProduct Applications: TECHNYL A 218W V30 Black FA is used in all sectors of industry, offering an excellent combination of thermal and mechanical properties. This grade is recommended for the production of mechanical components in permanent or intermittent contact with hot water: i.e. (electro-magnetic valves). This material restricts electrolytical corrosion and can be used as insulation material for electronic connectors. The values of properties are for black grade.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
ISO 527 Type 1A
Elongation at Break 4.0 %
4.0 %
ISO 527 Type 1A
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527 Type 1A
Flexural Strength 180 MPa
26100 psi
ISO 178
Flexural Modulus 6.40 GPa
928 ksi
ISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Constant 3.3
3.3
IEC 60250
Dissipation Factor 0.080
0.080
IEC 60250
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Copyright © lookpolymers.com All Rights Reserved