Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyketone , Polyaryletherketone (PAEK), Carbon Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear resistance, the resin also offers the outstanding combination of ultra-performance attributes commonly known for PEEK. These include: chemical resistance, mechanical strength and stiffness, even at elevated temperatures, as well as long-term and high-temperature thermal-oxidative stability. AV-742 SL30 is formulated with the ternary anti-friction/anti-wear additive system comprised of carbon fiber, graphite, and polytetrafluoroethylene (PTFE). It offers wear resistance performance comparable to PEEK grades with this modifier system while being more cost-effective. This high flowing (low viscosity) grade is designed for use in the injection molding of thin, intricate or complex shapes, or parts in otherwise challenging molding confiations. If the part geometry is such that low viscosity is not a processing necessity, it is recommended that the companion grade AV-722 SL30 be considered first to take advantage of the higher molecular weight of that grade, which results in greater wear resistance as well as better overall mechanical performance in terms of toughness-related properties. The resin can be melt processed using conventional equipment and techniques. Potential applications for AV-742 SL30 include bushings, bearings, wear strips, wear rings, rollers, and other parts used in sliding friction components. The resin is black in color in its natural state.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Water Absorption 0.030 %

@Time 86400 sec
0.030 %

@Time 24.0 hour
ASTM D570
Viscosity 270000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
270000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm

@Thickness 3.18 mm
0.0010 - 0.0030 in/in

@Thickness 0.125 in
5" x 0.5" x 0.125" bars; ASTM D955
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Thickness 3.18 mm
0.016 - 0.018 in/in

@Thickness 0.125 in
5" x 0.5" x 0.125" bars; ASTM D955
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 400 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 752 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 87
87
M-Scale; ASTM D785
Tensile Strength 143 MPa
20700 psi
5.0 mm/min; ASTM D638
Tensile Strength, Yield 156 MPa
22600 psi
ISO 527-2/1A/5
Elongation at Break 1.8 %
1.8 %
5.0 mm/min; ASTM D638
1.8 %
1.8 %
ISO 527-2/1A/5
Tensile Modulus 13.0 GPa
1890 ksi
5.0 mm/min; ASTM D638
15.5 GPa
2250 ksi
ISO 527-2/1A/1
Flexural Strength 203 MPa
29400 psi
ISO 178
211 MPa
30600 psi
ASTM D790
Flexural Modulus 10.4 GPa
1510 ksi
ASTM D790
13.2 GPa
1910 ksi
ISO 178
Compressive Strength 121 MPa
17500 psi
ASTM D695
Shear Strength 70.0 MPa
10200 psi
ASTM D732
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
4.10 J/cm
7.68 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 5.80 kJ/m²
2.76 ft-lb/in²
ISO 180
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 10.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
5.56 µin/in-°F

@Temperature -58.0 - 122 °F
TMA; ASTM E831
Specific Heat Capacity 1.25 J/g-°C

@Temperature 50.0 °C
0.299 BTU/lb-°F

@Temperature 122 °F
DSC
1.71 J/g-°C

@Temperature 200 °C
0.409 BTU/lb-°F

@Temperature 392 °F
DSC
Thermal Conductivity 0.340 W/m-K
2.36 BTU-in/hr-ft²-°F
ASTM E1530
Melting Point 343 °C
649 °F
Peak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 276 °C
529 °F
Annealed; ASTM D648
Glass Transition Temp, Tg 152 °C
306 °F
ASTM D3418
Processing Properties Metric English Comments
Rear Barrel Temperature 354 °C
669 °F
Middle Barrel Temperature 366 °C
691 °F
Front Barrel Temperature 371 °C
700 °F
Nozzle Temperature 374 °C
705 °F
Melt Temperature 366 - 388 °C
691 - 730 °F
Mold Temperature 149 - 177 °C
300 - 351 °F
Drying Temperature 149 °C
300 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Additive Carbon Fiber + Graphite + PTFE Lubricant
Appearance Black
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Flame Retardant
Good Chemical Resistance
Good Dimensional Stability
Good Wear Resistance
High Heat Resistance
Forms Pellets
Generic PAEK
Injection Rate Fast
Processing Method Injection Molding
Machining
Profile Extrusion
Screw Compression Ratio 2.0:1.0 to 3.0:1.0
Uses Automotive Applications
Bushings
Thin-walled Parts
Wear Strip