Flexural Strength 203 MPa
29400 psi
ASTM D-790
PlastiComp Complet® LGF20 - PA6 Nylon 6, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 20% long glass reinforcementInformation provided by PlastiComp, Inc.
Flexural Strength 203 MPa
29400 psi
ISO 178
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re..
Flexural Strength 203 MPa
29400 psi
ASTM D790
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughness-re..
Flexural Strength 203 MPa
29400 psi
ISO 178
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
AV-742 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wea..
Flexural Strength 203 MPa
29400 psi
ASTM D790
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK), 13% Glass Fiber
KetaSpire® KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughnes..
Flexural Strength 203 MPa
29400 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DF0089 PC
LNP THERMOCOMP* DF0089 is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features include: Flame Retardant.
Flexural Strength 203 MPa
29400 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DF008ER PC
LNP THERMOCOMP* DF008ER is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features include: Easy Molding, Mold Release.
Flexural Strength 203 MPa
29400 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PF006 PA 6
LNP THERMOCOMP* PF006 is a compound based on Nylon 6 resin containing 30% Glass Fiber.
Flexural Strength 203 MPa
29400 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF0049SP PA 66
LNP* THERMOCOMP* RF0049SP is a compound based on Nylon 66 containing 20% Glass Fiber. Added features of this grade include: Flame Retardant, Heat Stabilized.
Flexural Strength 203 MPa
29400 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DF008ERH PC
LNP THERMOCOMP* DF008ERH is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare.
Flexural Strength 203 MPa
29400 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PF006U PA 6
LNP THERMOCOMP* PF006U is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added features of thie grade are: UV Stabilized.
Flexural Strength 203 MPa
29400 psi
ISO 178
Polyplastics FR-PET® B9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
Information provided by PolyPlastics.
Flexural Strength 203 MPa
29400 psi
ISO 178
Polyplastics FR-PET® C9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
Information provided by PolyPlastics.
Flexural Strength 203 MPa
29400 psi
ASTM D790
A. Schulman ComAlloy Hiloy® 435 Glass/Mineral Reinforced, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Strength 203 MPa
29400 psi
ASTM D790
A. Schulman ComAlloy Hiloy® 610 Nylon 6, Glass/Mineral Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Strength 203 MPa
29400 psi
ASTM D790
A. Schulman ComAlloy Hiloy® 753 Glass Reinforced, Flow Enhanced, PPS Alloy, UL