Thermal Properties Metric English Comments
Glass Transition Temp, Tg 152 - 154 °C
306 - 309 °F
DSC/onset
Gharda Chemicals G-PAEK™ 1200FCM Ultra High Performance PEK Polymer  (discontinued **)
Milled carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in colorApplication Areas: Suitable for high temperature applica..
Glass Transition Temp, Tg 152 °C
306 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea..
Glass Transition Temp, Tg 152 °C
306 °F
ASTM D3418
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re..
Glass Transition Temp, Tg 152 °C
306 °F
ASTM D3418
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot..
Glass Transition Temp, Tg 152 °C
306 °F
ASTM D3418
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte..
Glass Transition Temp, Tg 152 °C
306 °F
ASTM D3418
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In..
Glass Transition Temp, Tg 152 °C
306 °F
Onset; ISO 11357
Victrex® HT™ P22 Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact compliantInfo..
Glass Transition Temp, Tg 152 °C
306 °F
Onset; ISO 11357
Victrex® HT™ P22PF Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, easy flow, FDA food contact compliantInfo..
Glass Transition Temp, Tg 152 °C
306 °F
Onset; ISO 11357
Victrex® HT™ P45 Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion compounding, low flow, FDA food contact compliant, co..
Glass Transition Temp, Tg 152 °C
306 °F
Onset; ISO 11357
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com..
Glass Transition Temp, Tg 152 °C
306 °F
Onset; ISO 11357
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp..
Glass Transition Temp, Tg 152 °C
306 °F
Onset; ISO 11357
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia..
Glass Transition Temp, Tg 152 °C
306 °F
Onset; ISO 11357
Victrex® WG102™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c..
Glass Transition Temp, Tg 152 - 154 °C
306 - 309 °F
DSC/onset
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:..
Glass Transition Temp, Tg 152 - 154 °C
306 - 309 °F
DSC/onset
Gharda Chemicals G-PAEKâ„¢ 1230CF Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic material, 30% carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in ..
Glass Transition Temp, Tg 152 - 154 °C
306 - 309 °F
DSC/onset
Gharda Chemicals G-PAEKâ„¢ 1230FC Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic material, 10% carbon fiber, 10% PTFE and 10% graphite reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection mo..
Glass Transition Temp, Tg 152 °C
306 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding..
Glass Transition Temp, Tg 152 °C
306 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
AV-742 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wea..
Glass Transition Temp, Tg 152 °C
306 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th..
Glass Transition Temp, Tg 152 °C
306 °F
DSC
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and ..
Glass Transition Temp, Tg 152 °C
306 °F
DSC
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide..
Glass Transition Temp, Tg 152 °C
306 °F
Wet
Hexcel® F161 Epoxy Resin
F161 is a structural, heat resistant and electrical grade epoxy formulation designed for autoclave curing. F161 is a high temperature, laminate grade epoxy resin with a 350ºF (177ºC) cure. F161 is..
Glass Transition Temp, Tg 152 °C
306 °F
Transition Temperature, tested in accordance with ASTM D1525; ASTM E1356
Entec Hylex® P1302B Polycarbonate
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Glass Transition Temp, Tg 152 - 154 °C
306 - 309 °F
DSC/onset
Gharda Chemicals G-PAEK™ 1200P Ultra High Performance PEK Polymer
Product Details: Ultra High performance thermoplastic material, unreinforced Poly Aryl Ether Ketone (G-PAEK), semi-crystalline, coarse powder for extrusion compounding, FDA food contact compliant, ..
Glass Transition Temp, Tg 152 - 154 °C
306 - 309 °F
DSC/onset
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige ..
Glass Transition Temp, Tg 152 °C
306 °F
Onset; ISO 11357
Victrex® HT™ G45 Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia..
Glass Transition Temp, Tg 152 °C
306 °F
Onset; ISO 11357
Victrex® HT™ P45PF Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact compliantInfor..