Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 4.00 hour | 4.00 hour | |
PolyOne Gravi-Tech™ GRV-NY-030-SS Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Dry Time | 4.00 hour | 4.00 hour | |
PolyOne Nymax™ 623 HS Black 13 1 Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Polymer Resources PC/TP-FR3 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
PolyOne Bergamid™ XP6042701 Polyamide 6 (Nylon 6) Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3.5 sec Cycle Time: 18 to 60 secInformation provided by PolyOne |
|||
Dry Time | 4.00 hour | 4.00 hour | |
PolyOne Edgetek® X TR2-10GF/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Celanese Celanex® 1400A PBT
(Unverified Data**) Celanex 1400A is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 1400A is a high flow material.Information provide.. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Celanese Celanex® 1700FC PBT
(Unverified Data**) Celanex 1700FC is a very high molecular weight extrusion grade of unreinforced polybutylene terephthalate for use in food contact applications.high molecular weight, unfilled PBT for use in food con.. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Celanese Celanex® 4306 PBT, 30% Glass Reinforced
(Unverified Data**) Celanex 4306 is a 30% glass reinforced, toughened, low warpage thermoplastic polyester.30% glass-fiber, impact modified, low warpInformation provided by Celanese |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Celanese Vandar® 4632Z PBT, 15% Glass Reinforced
(Unverified Data**) Vandar 4632Z is a high impact, 15% glass reinforced polyester alloy. It combines high strength and toughness with a moderate degree of rigidity. It is characterized by excellent solvent resistance, .. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS)
(Unverified Data**) EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491°F), E.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | DAM; Dehumidified Dryer; Extrusion |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h.. |
|||
Dry Time | 4.00 - 5.00 hour | 4.00 - 5.00 hour | Injection Molding |
LG Chemical LUMID GP3400A(W) PA6+MF40%, General Purpose Feature: Injection Molding, PA6+MF40%, General PurposeApplication: E&E (Rice Cooker Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
Dry Time | 4.00 - 5.00 hour | 4.00 - 5.00 hour | Injection Molding |
LG Chemical Lupox® GP2056F PBT+GF5% Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Dry Time | 4.00 - 5.00 hour | 4.00 - 5.00 hour | Injection Molding |
LG Chemical Lupox® LW5300M PBT+PC+MF30% Description: Injection Molding, PBT+PC+MF30%, Low WarpageApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 103598-77-2, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | Injection Molding |
LG Chemical LUPOY SR3108L PC, High Impact Description: Injection Molding, PC, High Flow, High Impact, White Color OnlyApplication: BLU Mold frame for Mobile DevicesCAS: 103598-77-2 and 13463-67-1Information provided by LG Chemical |
|||
Dry Time | 4.00 - 5.00 hour | 4.00 - 5.00 hour | |
Lubrizol Estane® S392A Thermoplastic Polyurethane Type: Estane® S392A is a Shore 93A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion, Blow .. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Eurostar Starflam AFR470X2 PA66, 35% Glass Filled, Injection Molded AFR470X2 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Eurostar Starflam RF0055E PA66/6, 25% Glass Filled, Injection Molded Starflam RF0055E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z250EM)Information provided by Polym.. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Eurostar Starflam PK0052E PA6, 25% Mineral Filled, Injection Molded PK0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Filed, Polyamide 6 Injection Molding (also known as PM3520Z222 or PA 25E6 U9 Z22)Information provided by Polymer Technolo.. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Eurotec® Tecopet® PT74 CR30 BK111 PR PET, 30% carbon fiber reinforced, black, fast crystallization grade Information provided by Eurotec® |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Celanese CELANEX 2401 MT PBT, Medical Technology Celanex 2401 MT Natural is an unreinforced, high molecular weight PBT that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Maste.. |
|||
Dry Time | 4.00 hour | 4.00 hour | Extrusion |
Alliance Polymers Zythane™ 5090A Thermoplastic Polyurethane Elastomer Zythane™ 5090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | Demold time, catalyzed with Moldmaster Blue |
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties .. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Arkema Group Rilsan® Clear G350 Polyamide Rilsan® Clear G350 is a high performance transparent polyamide. This grade has been specially designed for injection molding applications, ideally suited for optics as high end eyewear frames.Infor.. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Celanese Celstran® PP-GF30-0405 P10 PP, 30% Glass Reinforced Material code according to ISO 1043-1: PPInformation provided by Celanese |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Celanese VECTRA MT1310 LCP, 30% Medical Technology The Standard for the Industry. Excellent balance of properties, including easy flow, easy processing, thermal stability, chemical resistance, mechanical and electrical properties. Suitable for vapo.. |