Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better dimensiona.. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. .. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea.. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re.. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
(Unverified Data**) AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot.. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621.. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r.. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better di.. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res.. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK) AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding.. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK) AV-742 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wea.. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK) AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th.. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers Radel® R-7159 Polyphenylsulfone (PPSU) Radel® R-7159 polyphenylsulfone (PPSU) was developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical burn.. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers Radel® R-7400 Polyphenylsulfone (PPSU) Radel® R-7300 (for light colors) and R-7400 (for darker colors) polyphenylsulfone resins were developed specifically for aircraft interior applications, and through the use of a proprietary flame.. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers Radel® R-7535 Polyphenylsulfone (PPSU) Radel® R-7535 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications. This product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical bu.. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers Radel® R-7558 Polyphenylsulfone (PPSU) Radel® R-7558 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications. This product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical bu.. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers Radel® R-7625 Polyphenylsulfone (PPSU) Radel® R-7625 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications that offers improved UV resistance versus Radel® R-7535 and Radel® R-7558. The product .. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This resin ret.. |
|||
Melt Temperature | 366 - 388 °C | 691 - 730 °F | |
Solvay Specialty Polymers Radel® R-7300 Polyphenylsulfone (PPSU) Radel® R-7300 (for light colors) and R-7400 (for darker colors) polyphenylsulfone resins were developed specifically for aircraft interior applications, and through the use of a proprietary flame r.. |