Polymer Property : Specific Heat Capacity = 0.409 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.71 J/g-°C

@Temperature 200 °C
0.409 BTU/lb-°F

@Temperature 392 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re..
Specific Heat Capacity 1.71 J/g-°C

@Temperature 200 °C
0.409 BTU/lb-°F

@Temperature 392 °F
ASTM C351
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
AV-742 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wea..