Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.530 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ PPH-20G Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.530 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ 623 Zip 5 HS Black 13 Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Izod Impact, Notched | 0.530 J/cm @Thickness 3.17 mm |
0.993 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Trimid® N66-100L Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
PolyOne Edgetek® PS-30CF/000 HF UV BLACK Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.530 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Fittings 210A Gray 172(HS) Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Izod Impact, Notched | 0.530 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ DP 9052-3-1000 Polyethylene, High Density (HDPE) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to st.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP PFI12R PA 6 LNP* LUBRICOMP* PFI12R is a compound based on Nylon 6 resin containing 10% Glass Fiber, 2% Silicone. Added features of this material include: Wear Resistant, Mold Release. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature 23.0 °C |
0.993 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 1000M PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature -30.0 °C |
0.993 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM HU2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral aci.. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature 23.0 °C |
0.993 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp AF008 ABS (Asia Pacific) LNP* Thermocomp* AF008 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature 23.0 °C |
0.993 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly (Asia Pacific) LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP KFB11 Acetal Copoly LNP* THERMOCOMP* KFB11 is a compound based on Acetal Copolymer resin containing 5% Glass Fiber, 5% Glass Bead. Added features of this material include: Low Warpage, Chemically Coupled. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature 23.0 °C |
0.993 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon WFD059 PBT LNP* Stat-kon* WFD059 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature 23.0 °C |
0.993 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp MF006S PP (Asia Pacific) LNP* Thermocomp* MF006S is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia P.. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature 23.0 °C |
0.993 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp P1000P PA 6 LNP* Thermocomp* P1000P is a compound based on Nylon 6 resin. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1245 is a 20% CAC03 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1245U CaCO3 Filled UV Stable Copolymer Polypropylene DescriptionPolyfort® FPP 1245U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.530 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers NYLON 66 Natural Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
Eurostar Starflam PZ0052E PA6, 25% Glass Filled, Injection Molded PZ0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1005Z222 or PA625GFUZ22)Information provided by Polymer Technolo.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
Bapolene® PP5061 Polypropylene, Injection Grade Bapolene PP5061 is a PP Random Copolymer for injection molding. This resin exhibits good clarity and impact properties. This product meets FDA standards for food contact applications.Applications:.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 528LW Nylon 66 General purpose injection molding grade.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 412 Polyester - PBT, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Voloy® 431 Glass/Mineral Reinforced, PET Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 462 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 164 Polypropylene, Mineral Reinforced, Chemically Coupled, Impact Modified Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Izod Impact, Notched | 0.530 J/cm @Thickness 3.17 mm |
0.993 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Performance Polymers IPS II PPL-C4050 PEKK (Polyetherketoneketone) Linear Molding Grade Amber pellets; neat resinInformation provided by Infinite Polymer System II. |