Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 152 - 154 °C | 306 - 309 °F | DSC/onset |
Gharda Chemicals G-PAEK™ 1200FCM Ultra High Performance PEK Polymer
(discontinued **) Milled carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in colorApplication Areas: Suitable for high temperature applica.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | DSC |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
(Unverified Data**) AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | Onset; ISO 11357 |
Victrex® HT™ P22 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact compliantInfo.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | Onset; ISO 11357 |
Victrex® HT™ P22PF Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, easy flow, FDA food contact compliantInfo.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | Onset; ISO 11357 |
Victrex® HT™ P45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion
compounding, low flow, FDA food contact compliant, co.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | Onset; ISO 11357 |
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | Onset; ISO 11357 |
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | Onset; ISO 11357 |
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | Onset; ISO 11357 |
Victrex® WG102™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c.. |
|||
Glass Transition Temp, Tg | 152 - 154 °C | 306 - 309 °F | DSC/onset |
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:.. |
|||
Glass Transition Temp, Tg | 152 - 154 °C | 306 - 309 °F | DSC/onset |
Gharda Chemicals G-PAEKâ„¢ 1230CF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in .. |
|||
Glass Transition Temp, Tg | 152 - 154 °C | 306 - 309 °F | DSC/onset |
Gharda Chemicals G-PAEKâ„¢ 1230FC Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 10% carbon fiber, 10% PTFE and 10% graphite reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection mo.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | DSC |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK) AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | DSC |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK) AV-742 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wea.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | DSC |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK) AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and .. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | Wet |
Hexcel® F161 Epoxy Resin F161 is a structural, heat resistant and electrical grade epoxy formulation designed for autoclave curing. F161 is a high temperature, laminate grade epoxy resin with a 350ºF (177ºC) cure. F161 is.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | Transition Temperature, tested in accordance with ASTM D1525; ASTM E1356 |
Entec Hylex® P1302B Polycarbonate Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Glass Transition Temp, Tg | 152 - 154 °C | 306 - 309 °F | DSC/onset |
Gharda Chemicals G-PAEK™ 1200P Ultra High Performance PEK Polymer Product Details: Ultra High performance thermoplastic material, unreinforced Poly Aryl Ether Ketone (G-PAEK), semi-crystalline, coarse powder for extrusion compounding, FDA food contact compliant, .. |
|||
Glass Transition Temp, Tg | 152 - 154 °C | 306 - 309 °F | DSC/onset |
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige .. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | Onset; ISO 11357 |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |
|||
Glass Transition Temp, Tg | 152 °C | 306 °F | Onset; ISO 11357 |
Victrex® HT™ P45PF Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact compliantInfor.. |