Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.47 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
PolyOne Geon™ Vinyl Wire & Cable WJAX204V Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Specific Gravity 1.47 g/cc
1.47 g/cc
CMC form; ASTM D792
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, C2 Reinforced
Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel..
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Quadrant EPP Acetron® MD Metal-detectable Copolymer Acetal (ASTM Product Data Sheet)
Low moisture absorption High strength, stiffness Easy to machine No centerline porosity in Acetron® GP Many formulation options: Copolymer, Homopolymer, PTFE filled, and Internally lubricated/enha..
Specific Gravity 1.47 g/cc
1.47 g/cc
Radici Radilon® S CP400 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
PolyOne Geon™ Vinyl Flexible R 960A Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Celanese FORTRON 1120L4 PPS, 20% Specialty  (Unverified Data**)
Fortron 1120L4 is a 20% glass fiber reinforced injection molding grade exhibiting excellent heat and chemical resistance, inherent flame retardancy, high hardness and stiffness at elevated temperatu..
Specific Gravity 1.47 g/cc
1.47 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1301-8386 PPS, linear, with aramid reinforcement and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma..
Specific Gravity 1.47 g/cc
1.47 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 2205-7123 Blend based on polyaryl ether ketone, with carbon fiber, PTFE, lubricant modified
Applications: High dimensionally stable precision parts, high continuous use temperature.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceChemical and hydr..
Specific Gravity 1.47 g/cc
1.47 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 80-7050 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
LG Chemical Lupox® GP2056F PBT+GF5%
Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
Specific Gravity 1.47 - 1.53 g/cc
1.47 - 1.53 g/cc
ASTM D 792
Karina 806-40/236-H-ISE-LMP White PVC Compound
Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.47 - 1.53 g/cc
1.47 - 1.53 g/cc
NBR NM-IEC 60811-1-3
Karina E 10/85-FC-LMP White Color Concentrate for PVC
Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con..
Specific Gravity 1.47 g/cc
1.47 g/cc
Sylvin Technologies 8960-90 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC
LNP* Lubricomp* Lexan_LF1520A compound is a 20% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances.
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Europe-Africa-Middle East)
LNP* Lubricomp* Lexan_FL1520 compound is a 20% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances.
Specific Gravity 1.47 g/cc
1.47 g/cc
Silberline Aquasil® "BP" 5745
Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and ..
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP XFL36 AMORPHOUS POLYAMIDE
LNP* LUBRICOMP* XFL36 is a compound based on Amorphous Nylon containing 30% Glass Fiber and 15% PTFE. Added feature of this material is: Wear Resistant.
Specific Gravity 1.47 g/cc
1.47 g/cc
Silberline Sparkle Silver® 3000-AR
Sparkle Silver® 3000-AR is a medium, high sparkle, brilliant, non-leafing aluminum pigment popular for solvent Automotive Applications. It shows exceptional resistance to spotting when incorporat..
Specific Gravity 1.47 g/cc
1.47 g/cc
Silberline Stamford "O" Standard Series
Stamford O is a fine, non-leafing aluminum pigment with good opacity for solvent based industrial coatings. This is an economical grade with cornflake geometry and wide particle size distribution ra..
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D795
Saint-Gobain Meldin® 1380 Thermoplastic Bearing Material
Specify Meldin 1380 for use with soft mating surfaces that gall easily, such as stainless steel or aluminum. Meldin 1380 also complies with the FDA Title 21 CFR regulations for contact with article..
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
A. Schulman POLYBATCH™ Gold 7060E POLYBATCH® Concentrate Based In LDPE
Description POLYBATCH® 7060E is a gold color concentrate based in LDPE. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 7060E is heavy meta..
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Colorite Polymers 7884H General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Specific Gravity 1.47 g/cc
1.47 g/cc
uncatalyzed, Deep Section Catalyst
ACC QSil 940 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting
QSil 940 is a special purpose, two-component condensation cure siloxane elastomer that exhibits excellent release properties unless a primer is used which results in excellent adhesion. The material..
Specific Gravity 1.47 g/cc
1.47 g/cc
Aremco Corr-Paint™ CP4060-S High Temperature Protective Coating, Silicone-Polyester
Specific Gravity 1.47 - 1.51 g/cc
1.47 - 1.51 g/cc
ASTM D-792
Axiall 8864 Moldings & Extrusions Flexible PVC
General purpose PVC extrusion compound recommended for applications that require UV and fungus resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.47 - 1.51 g/cc
1.47 - 1.51 g/cc
ASTM D-792
Axiall 38831 Coax & Telecom Flexible PVC
Category 5(+), flexible CMR jacket at 28-30 mils over HDPE inners.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
A. Schulman POLYBATCH™ Gold 7060E POLYBATCH® Concentrate Based In LDPE
Description POLYBATCH® 7060E is a gold color concentrate based in LDPE. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 7060E is heavy meta..
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
PolyOne Edgetek® AT-10GF/000 FDA Acetal-Copolymer, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedFDA CapablePolyOne First ChoiceInformation provided by PolyOne Corporation.
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D 792
SABIC Innovative Plastics Valox® VSR4150 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D 792
RTP Company RTP PA6 40 GF BLK Nylon 6 (PA) Value Product - Glass Fiber - Heat Stabilized