Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
8HS form; ASTM D792
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, ENKA Reinforced
Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel..
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Polymer Resources AH-GP2-TFE10 Acetal Homopolymer, 10% PTFE
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
PolyOne Geon™ Vinyl Flexible D8500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
PolyOne Geon™ Vinyl Flexible FC900 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
LNP VALOX® SMV5846 PBT + PET Alloy, 20% Carbon Fiber Reinforcement  (discontinued **)
ESD ApplicationsFeatures: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is ..
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re..
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D 792
RTP Company RTP 800 TFE 15 SI 2 Z Acetal (POM), PTFE & Silicone Lubricated - FDA Compliant Ingredients
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
RTP Company RTP 4300 B-322  Polysulfone/Polycarbonate Alloy (PSU/PC) Glass Fiber 22% - Flame Retardant
Glass Fiber 22% - Flame RetardantComments:Glass FiberFlame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information ..
Specific Gravity 1.47 g/cc
1.47 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1700-8019 PPO, with glass fiber and PTFE, low-warpage
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Improved friction and wear behaviour...
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Fiberfil® J-60/30/FR Polypropylene Homopolymer, 30% Glass Fiber Reinforced, Flame Retardant
Information provided by FIBERFIL Engineered Plastics
Specific Gravity 1.47 - 1.53 g/cc
1.47 - 1.53 g/cc
ASTM D 792
Karina 806-18/364-BY-ERYB Gray PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.47 - 1.53 g/cc
1.47 - 1.53 g/cc
NBR 14288
Karina 828-08/20-AY-ERYB Beige PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.47 - 1.53 g/cc
1.47 - 1.53 g/cc
ASTM D 792
Karina 850-10/99-Y-ERYB White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.47 - 1.53 g/cc
1.47 - 1.53 g/cc
NBR NM-IEC 60811-1-3
Karina E 32/1-FC-LMP Orange Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
Specific Gravity 1.47 g/cc
1.47 g/cc
Sylvin Technologies 8960-90 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Specific Gravity 1.47 g/cc
1.47 g/cc
Sylvin Technologies 9077-75C Natural PVC for Injection Molding
Information provided by Sylvin Technologies Inc.
Specific Gravity 1.47 g/cc
1.47 g/cc
+.02
Spartech E65695 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP XFL36 AMORPHOUS POLYAMIDE
LNP* LUBRICOMP* XFL36 is a compound based on Amorphous Nylon containing 30% Glass Fiber and 15% PTFE. Added feature of this material is: Wear Resistant.
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Shinkong Synthetic Fibers Shinite® D201M20 PBT, 20% Mineral Filled
Information from Shinkong Synthetic Fibers Corp.
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
A. Schulman POLYBATCH™ Gold 7060E POLYBATCH® Concentrate Based In LDPE
Description POLYBATCH® 7060E is a gold color concentrate based in LDPE. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 7060E is heavy meta..
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
A. Schulman POLYBATCH™ Gold 7060E POLYBATCH® Concentrate Based In LDPE
Description POLYBATCH® 7060E is a gold color concentrate based in LDPE. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 7060E is heavy meta..
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D 792
RTP Company ESD C 280 FR Nylon 6/6 (PA); Carbon Fiber - Flame Retardant - ESD Protection - Electrically Conductive
Specific Gravity 1.47 g/cc
1.47 g/cc
uncatalyzed, Deep Section Catalyst
ACC QSil 940 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting
QSil 940 is a special purpose, two-component condensation cure siloxane elastomer that exhibits excellent release properties unless a primer is used which results in excellent adhesion. The material..
Specific Gravity 1.47 g/cc
1.47 g/cc
ISO 1183
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, Conditioned
Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters..
Specific Gravity 1.47 g/cc
1.47 g/cc
Aremco Ceramabind™ 542 High Temperature Inorganic Binder
Single part, low viscosity, water-dispersed, aluminum phosphate solution for penetrating ultra fine thermal spray applications to 3000°F (1650°C).
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D-792
Axiall 7555 Rigid PVC, Extrusion, White
Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn..
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D-792
Axiall 8150 Rigid PVC, Extrusion & Molding
Georgia Gulf 8150 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical Resista..
Specific Gravity 1.47 g/cc
1.47 g/cc
uncatalyzed, Deep Section Catalyst
ACC QSil 58 QSI Quantum Silicones 50 Durometer Condensation Cure for Potting
QSil 58 is a red, high temperature, self-leveling, two-component silicone material primarily used for potting applications. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section C..
Specific Gravity 1.47 g/cc
1.47 g/cc
ISO 1183
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM
Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters..
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D 792
SABIC Innovative Plastics Valox® VSR4150 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.