Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.0 GPa | 1890 ksi | ASTM D638 |
Premix Premi-Glas® 3101-20 Polyester BMC Premi-Glas® 3101-20 a 20% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL 94-.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527 |
Nilit FRIANYL A63 GV40 Nylon 6.6 for injection molding, 40% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 370 /B AV2 370 PET-35% Glass Reinforced (European and Asian Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | 5.0 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-1/-2 |
DSM Akulon® K224-HG8 Nylon 6-40% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG45-AS00N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG45-B100N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527 |
Grupo Repol Dinalon® A1S25 G45 H PA66 45% Glass Fiber, Heat Stabilized Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V40 Black 21 NHFE PA66, 40% glass fiber, DRY Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 40% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V40 PA66, 40% glass fiber, DRY Description: Polyamide PA66, reinforced with 40% of glass fiber, heat stabilized for injection molding.Available in: Asia Pacific, Europe and North AmericaProduct Applications: TECHNYL A 218 V40 is .. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ASTM D638 |
Solvay Technyl® A 216 V40 40% Glass Filled Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-1 |
Vyncolit X7012 Glass Fiber Reinforced Novolac Phenolic Novolac resin based, glass fiber and glass beads reinforced. High mechanical strength even at high temperatures in Long Life CoolantsInformation provided by Sumitomo Bak North America, Inc. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 1SVX-50H nat PA1010-GF50 Product Description: Grilamid 1SVX-50H natural is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-4 FWA black 9225 PA*-GF40 Product description: Grivory GV-4 FWA black 9225 is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-4 FWA nat PA*-GF40 Product description: Grivory GV-4 FWA natural is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 3915 PA12-GF50 Product description: Grilamid XE 3915 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following produce profile:Good UV StabilityHigh impact strengthVe.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FG70G50HSLA BK309 Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 370 XT PET-GF35 35% Glass Reinforced, Applications with extremely narrow tolerances |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 372 PET-35% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | 1 [mm/min]; ISO 527-2/1 |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Conditioned, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® TS200B3 PA46-CF15 15% Carbon Reinforced |
|||
Tensile Modulus | 13.0 - 15.0 GPa | 1890 - 2180 ksi | ISO 527 |
Vyncolit 3520 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1625 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1625 HS is a 25% carbon and glass-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This material is .. |