Polymer Property : Izod Impact, Notched = 7.68 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.10 J/cm
7.68 ft-lb/in
ASTM D4812
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re..
Izod Impact, Notched 4.10 J/cm
7.68 ft-lb/in
ASTM D256
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a low ..
Izod Impact, Notched 4.10 J/cm
7.68 ft-lb/in
ASTM D256
Spartech Royalite R21M General Purpose ABS Resin
Data provided by the manufacturer. A general-purpose ABS resin with high impact strength, R-21M is a popular choice for a variety of products, from bicycle helmets and carrying cases to portable ta..
Izod Impact, Notched 4.10 J/cm
7.68 ft-lb/in
ASTM D256
Styrolution Terluran® SP-6 ABS
Description: High impact grade, suitable for extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Izod Impact, Notched 4.10 J/cm
7.68 ft-lb/in
ASTM D256
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of ..
Izod Impact, Notched 4.10 J/cm
7.68 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON RV00CEXS PA 66
LNP* VERTON* RV00CEXS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural.