Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 149 - 177 °C | 300 - 350 °F | |
Oxford Polymers PEEK 450-INJ-Black PEEK Product Description: Polyetheretherketone, general purpose injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Carbon black Special Characteristics: Precol.. |
|||
Mold Temperature | 149 - 220 °C | 300 - 428 °F | Average value: 181 °C Grade Count:7 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Mold Temperature | 149 - 232 °C | 300 - 450 °F | Average value: 204 °C Grade Count:5 |
Overview of materials for PEKK, Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Mold Temperature | 149 - 171 °C | 300 - 340 °F | |
LNP Lubricomp® UFL-4036 HS Polyphthalamide, Glass Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr.. |
|||
Mold Temperature | 149 - 177 °C | 300 - 351 °F | |
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better dimensiona.. |
|||
Mold Temperature | 149 - 177 °C | 300 - 351 °F | |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea.. |
|||
Mold Temperature | 149 - 177 °C | 300 - 351 °F | |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re.. |
|||
Mold Temperature | 149 - 177 °C | 300 - 351 °F | |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
(Unverified Data**) AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot.. |
|||
Mold Temperature | 149 - 163 °C | 300 - 325 °F | |
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boil.. |
|||
Mold Temperature | 149 - 163 °C | 300 - 325 °F | |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral acids... |
|||
Mold Temperature | 149 - 163 °C | 300 - 325 °F | |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn.. |
|||
Mold Temperature | >= 149 °C | >= 300 °F | |
PolyOne Lubri-Tech™ SF-10CF/15T Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced, PTFE Lubricated
(discon Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 149 - 177 °C | 300 - 351 °F | |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621.. |
|||
Mold Temperature | 149 - 177 °C | 300 - 351 °F | |
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better di.. |
|||
Mold Temperature | 149 - 177 °C | 300 - 351 °F | |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK) AV-742 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wea.. |
|||
Mold Temperature | 149 - 163 °C | 300 - 325 °F | |
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU) Veradel® 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, .. |
|||
Mold Temperature | 149 - 163 °C | 300 - 325 °F | |
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac.. |
|||
Mold Temperature | 149 - 163 °C | 300 - 325 °F | |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac.. |
|||
Mold Temperature | 149 - 163 °C | 300 - 325 °F | |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU) Veradel® 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to s.. |
|||
Mold Temperature | 149 - 163 °C | 300 - 325 °F | |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral aci.. |
|||
Mold Temperature | 149 - 163 °C | 300 - 325 °F | |
Solvay Specialty Polymers Veradel® AG-320 Polyethersulfone (PESU), 20% Glass Fiber Veradel® AG-320 is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Mold Temperature | 149 - 177 °C | 300 - 350 °F | |
Bulk Molding Compounds BMC 304 Automotive Grade Molding Compound BMC 304 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 304 can be coated using traditional or electrostatic coati.. |
|||
Mold Temperature | 149 - 177 °C | 300 - 351 °F | |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |
|||
Mold Temperature | 149 - 163 °C | 300 - 325 °F | |
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU)
(Unverified Data**) Veradel 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |
|||
Mold Temperature | 149 - 163 °C | 300 - 325 °F | |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. .. |
|||
Mold Temperature | 149 - 163 °C | 300 - 325 °F | |
Solvay Specialty Polymers Veradel® AG-320 Polyethersulfone (PESU)
(Unverified Data**) Veradel AG-320 is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |
|||
Mold Temperature | 149 - 163 °C | 300 - 325 °F | |
Solvay Specialty Polymers Veradel® AG-330 Polyethersulfone (PESU)
(Unverified Data**) Veradel AG-330 is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |
|||
Mold Temperature | 149 - 232 °C | 300 - 450 °F | |
RTP Company RTP 4105 Polyetherketoneketone (PEKK), Glass Fiber |
|||
Mold Temperature | 149 - 232 °C | 300 - 450 °F | |
RTP Company RTP 3100 Perfluoroalkoxy (PFA) Base Resin
(discontinued **) Base ResinComments:UnfilledUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this pro.. |
|||
Mold Temperature | 149 - 171 °C | 300 - 340 °F | |
LNP Lubricomp® BGU- Polyphthalamide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr.. |