Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Category : Polyaryletherketone (PAEK), Carbon Fiber Filled Product List

Tips: 50 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO. Manufacturer Trade Name
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
Gharda Chemicals G-PAEK™ 1200FCM Ultra High Performance PEK Polymer  (discontinued **)
RTP Company RTP 3883 Polyaryletherketone (PAEK), Carbon Fiber 20%  (discontinued **)
RTP Company RTP 3885 Polyaryletherketone (PAEK), Carbon Fiber 30%  (discontinued **)
RTP Company RTP 3887 Polyaryletherketone (PAEK), Carbon Fiber 40%  (discontinued **)
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)  (Unverified Data**)
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
Lehmann & Voss LUVOCOM® 1114-8364 PAEK, with carbon fiber, PTFE, lubricant modified Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 2205-7123 Blend based on polyaryl ether ketone, with carbon fiber, PTFE, lubricant modified Lehmann & Voss & Co. LUVOCOM®
Gharda Chemicals G-PAEKâ„¢ 1230CF Ultra High Performance PEK Polymer Gharda Chemicals G-PAEK™
Gharda Chemicals G-PAEKâ„¢ 1230FC Ultra High Performance PEK Polymer Gharda Chemicals G-PAEK™
Lehmann & Voss LUVOCOM® 1114-0717 PAEK, with carbon fiber and PTFE Lehmann & Voss & Co. LUVOCOM®
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber Solvay Specialty Polymers AvaSpire®
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber Solvay Specialty Polymers AvaSpire®
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber Solvay Specialty Polymers AvaSpire®
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK) Solvay Specialty Polymers AvaSpire®
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK) Solvay Specialty Polymers AvaSpire®
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK) Solvay Specialty Polymers AvaSpire®
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber Solvay Specialty Polymers AvaSpire®
Ensinger Tecapeek® Classix Polyaryletherketone (PAEK) Ensinger Tecapeek®
Ensinger TECATEC™ CF60 Polyaryletherketone (PAEK) Ensinger TECATEC™
RTP Company RTP 3881 Polyaryletherketone (PAEK), Carbon Fiber 10%  (discontinued **)
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
Copyright © lookpolymers.com All Rights Reserved