Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.22 - 1.91 g/cc
0.0441 - 0.0690 lb/in³
Average value: 1.47 g/cc Grade Count:89
Filler Content 5.00 - 76.0 %
5.00 - 76.0 %
Average value: 32.1 % Grade Count:56
Water Absorption 0.120 - 0.400 %
0.120 - 0.400 %
Average value: 0.296 % Grade Count:18
Additive Loading 20.0 - 40.0 %
20.0 - 40.0 %
Average value: 30.0 % Grade Count:4
Linear Mold Shrinkage 0.000500 - 0.0160 cm/cm
0.000500 - 0.0160 in/in
Average value: 0.00227 cm/cm Grade Count:62
Linear Mold Shrinkage, Transverse 0.000500 - 0.00500 cm/cm
0.000500 - 0.00500 in/in
Average value: 0.00188 cm/cm Grade Count:6
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119 - 125
119 - 125
Average value: 122 Grade Count:4
Hardness, Shore A 70.0 - 99.0
70.0 - 99.0
Average value: 85.4 Grade Count:11
Hardness, Shore D 50.0 - 75.0
50.0 - 75.0
Average value: 65.4 Grade Count:22
Tensile Strength, Ultimate 14.5 - 1000 MPa
2100 - 145000 psi
Average value: 144 MPa Grade Count:84
24.0 - 102 MPa

@Temperature 0.000 - 60.0 °C
3480 - 14800 psi

@Temperature 32.0 - 140 °F
Average value: 54.9 MPa Grade Count:3
24.0 - 102 MPa

@Strain 2.00 - 30.0 %
3480 - 14800 psi

@Strain 2.00 - 30.0 %
Average value: 54.9 MPa Grade Count:3
Tensile Strength, Yield 49.0 - 227 MPa
7100 - 32900 psi
Average value: 137 MPa Grade Count:11
Elongation at Break 1.00 - 430 %
1.00 - 430 %
Average value: 15.4 % Grade Count:82
Elongation at Yield 1.60 - 190 %
1.60 - 190 %
Average value: 33.5 % Grade Count:7
Modulus of Elasticity 0.345 - 45.0 GPa
50.0 - 6530 ksi
Average value: 9.83 GPa Grade Count:74
Flexural Yield Strength 13.8 - 1150 MPa
2000 - 167000 psi
Average value: 254 MPa Grade Count:71
Flexural Modulus 0.234 - 45.0 GPa
33.9 - 6530 ksi
Average value: 9.38 GPa Grade Count:74
Compressive Yield Strength 8.27 - 440 MPa
1200 - 63800 psi
Average value: 98.9 MPa Grade Count:5
Izod Impact, Notched 0.427 - 5340 J/cm
0.800 - 10000 ft-lb/in
Average value: 4.92 J/cm Grade Count:65
2.00 - 4.00 J/cm

@Temperature -40.0 - -20.0 °C
3.75 - 7.49 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 3.00 J/cm Grade Count:1
Izod Impact, Unnotched 2.14 - 5340 J/cm
4.00 - 10000 ft-lb/in
Average value: 12.1 J/cm Grade Count:59
3.20 - 8.54 J/cm

@Temperature -40.0 - -40.0 °C
5.99 - 16.0 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 5.00 J/cm Grade Count:4
3.20 - 8.54 J/cm

@Thickness 3.20 - 81.3 mm
5.99 - 16.0 ft-lb/in

@Thickness 0.126 - 3.20 in
Average value: 5.00 J/cm Grade Count:4
Izod Impact, Notched (ISO) 33.5 - 33.5 kJ/m²

@Temperature -30.0 - -30.0 °C
15.9 - 15.9 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 33.5 kJ/m² Grade Count:1
Charpy Impact Unnotched 10.0 - 1000 J/cm²
47.6 - 4760 ft-lb/in²
Average value: 15.4 J/cm² Grade Count:12
6.50 - 16.0 J/cm²

@Temperature -40.0 - -20.0 °C
30.9 - 76.1 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 9.56 J/cm² Grade Count:11
Charpy Impact, Notched 3.00 - 7.00 J/cm²
14.3 - 33.3 ft-lb/in²
Average value: 4.84 J/cm² Grade Count:16
0.600 - 3.00 J/cm²

@Temperature -30.0 - -30.0 °C
2.86 - 14.3 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.30 J/cm² Grade Count:10
Dart Drop, Total Energy 17.0 - 31.0 J
12.5 - 22.9 ft-lb
Average value: 27.0 J Grade Count:4
14.0 - 25.0 J

@Temperature -29.0 - -29.0 °C
10.3 - 18.4 ft-lb

@Temperature -20.2 - -20.2 °F
Average value: 18.3 J Grade Count:4
Thermal Properties Metric English Comments
CTE, linear 9.00 - 162 µm/m-°C
5.00 - 90.0 µin/in-°F
Average value: 46.3 µm/m-°C Grade Count:23
Thermal Conductivity 0.231 - 0.403 W/m-K
1.60 - 2.80 BTU-in/hr-ft²-°F
Average value: 0.323 W/m-K Grade Count:5
Melting Point 190 °C
374 °F
Average value: 190 °C Grade Count:3
Maximum Service Temperature, Air 80.0 - 90.0 °C
176 - 194 °F
Average value: 87.5 °C Grade Count:4
Deflection Temperature at 0.46 MPa (66 psi) 104 - 170 °C
220 - 338 °F
Average value: 133 °C Grade Count:22
Deflection Temperature at 1.8 MPa (264 psi) 54.4 - 185 °C
130 - 365 °F
Average value: 102 °C Grade Count:54
Vicat Softening Point 87.0 - 186 °C
189 - 367 °F
Average value: 151 °C Grade Count:9
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Average value: -30.0 °C Grade Count:3
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:38
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+11 - 1.00e+16 ohm-cm
1.00e+11 - 1.00e+16 ohm-cm
Average value: 5.56e+14 ohm-cm Grade Count:18
Dielectric Constant 3.60 - 4.90
3.60 - 4.90
Average value: 4.33 Grade Count:7
Dielectric Strength 14.2 - 19.7 kV/mm
360 - 500 kV/in
Average value: 17.0 kV/mm Grade Count:7
Dissipation Factor 0.00300 - 0.0200
0.00300 - 0.0200
Average value: 0.0136 Grade Count:7
Processing Properties Metric English Comments
Processing Temperature 70.0 - 265 °C
158 - 509 °F
Average value: 198 °C Grade Count:43
Nozzle Temperature 221 - 249 °C
430 - 480 °F
Average value: 238 °C Grade Count:8
Die Temperature 245 - 260 °C
473 - 500 °F
Average value: 253 °C Grade Count:5
Melt Temperature 70.0 - 260 °C
158 - 500 °F
Average value: 229 °C Grade Count:43
Mold Temperature 20.0 - 121 °C
68.0 - 250 °F
Average value: 68.0 °C Grade Count:72
Injection Velocity 50.8 - 76.2 mm/sec
2.00 - 3.00 in/sec
Average value: 63.5 mm/sec Grade Count:5
Drying Temperature 80.0 - 132 °C
176 - 270 °F
Average value: 100 °C Grade Count:42
Moisture Content 0.0100 - 0.0500 %
0.0100 - 0.0500 %
Average value: 0.0181 % Grade Count:31
Dew Point -40.0 - -28.9 °C
-40.0 - -20.0 °F
Average value: -38.6 °C Grade Count:24
Injection Pressure 4.96 - 103 MPa
720 - 15000 psi
Average value: 83.0 MPa Grade Count:51