Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 3.00 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
North Wood Plastics Polypropylene with 20% Wood Fiber, Molding Grade
Data provided by North Wood Plastics, Inc.
Izod Impact, Unnotched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 1302 TFE 20  Polyphenylene Sulfide (PPS) Glass Fiber 15% - PTFE 20%  (discon
Glass Fiber 15% - PTFE 20%Comments:Glass FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provide..
Izod Impact, Unnotched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 1387 HM  Polyphenylene Sulfide (PPS) Carbon Fiber 40% - High Modulus  (disco
Carbon Fiber 40% - High ModulusComments:Carbon FiberHigh ModulusUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information prov..
Izod Impact, Unnotched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company ESD C 4005A  Polyphthalamide - Hot Water Mold (PPA) Conductive - Glass Fiber 30% &nbs
Conductive - Glass Fiber 30%Comments:ConductiveESD ProtectionGlass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Informat..
Izod Impact, Unnotched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 401 HI Polystyrene (PS), High Impact - Glass Fiber
Izod Impact, Unnotched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 4701 FR  Polytrimethylene Terephthalate (PTT) Glass Fiber 10% - Flame Retardant &
Glass Fiber 10% - Flame RetardantComments:Glass FiberFlame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information ..
Izod Impact, Unnotched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 4701 FR NH  Polytrimethylene Terephthalate (PTT) Glass Fiber 10% - Non Halogen Flame Retardant
Glass Fiber 10% - Non Halogen Flame RetardantComments:Glass FiberFlame RetardantHalogen FreeUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect..
Izod Impact, Unnotched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Ineos Nova Zylar® 221 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features: High clarityEnhanced mold releaseGood elongationStyrenic processing advantagesExcellent property retention after ETO and gamma sterilization Applications: DisplaysMedical devicesOffice acc..
Izod Impact, Unnotched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 1807  Acrylic (PMMA) Glass Fiber 40%  (discontinued **)
Glass Fiber 40%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Izod Impact, Unnotched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 3049  Polymethylpentene (PMP) Mineral 25%  (discontinued **)
Mineral 25%Comments:MineralUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this pro..
Izod Impact, Unnotched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 3499-3 X 91193 B  Liquid Crystal Polymer (LCP) Electronic Encapsulation - Thermally Conductive
Electronic Encapsulation - Thermally ConductiveComments:Encapsulation GradeThermally ConductiveUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can aff..
Izod Impact, Unnotched 1.60 - 8.00 J/cm
3.00 - 15.0 ft-lb/in
Average value: 4.41 J/cm Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor..
Izod Impact, Unnotched 1.60 - 6.40 J/cm
3.00 - 12.0 ft-lb/in
Average value: 2.81 J/cm Grade Count:25
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..
Izod Impact, Unnotched 1.60 J/cm
3.00 ft-lb/in
J/cm²; ISO 180A
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide Compound  (Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® R-7-120BL is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good weldline strength and low maintenance molding using..
Izod Impact, Unnotched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Electrablend® ABS CF10 FR BK 10% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Electrablend® ABS CF5 5% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 5% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)
Torlon® 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon® PAI h..
Izod Impact, Unnotched 1.60 - 2.14 J/cm

@Thickness 3.17 mm
3.00 - 4.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® ASA GF20 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites..
Izod Impact, Unnotched 1.60 J/cm

@Temperature -40.0 °C
3.00 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Spartech Noryl® SP-5210 Specialty Sheet
Description: Specialty SheetNoryl is a registered trademark of General Electric Company.Information provided by Spartech.
Izod Impact, Unnotched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Spartech Royalstatâ„¢ R635 ABS/Polyolefin Static Control Sheet
Description: Static Control SheetInformation provided by Spartech.
Izod Impact, Unnotched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Electrablend® ABS SS16 FR BK 16% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 16% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation provided by TP Composi..
Izod Impact, Unnotched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Daikin POLYFLON F-302 PTFE Fine Powder
Processing Methods: Paste extrusion.Applications: Small to large diameter tubes, flexible hoses, shrinkable tubes, heavy duty electric wires smaller than AGW18, and jackets.Information provided by ..
Izod Impact, Unnotched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Daikin POLYFLON MG-1030 PTFE 15% Glass Fiber Filled Molding Powder
15% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,..
Izod Impact, Unnotched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Daikin POLYFLON MG-1050F PTFE 25% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow
25% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl..
Izod Impact, Unnotched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Daikin POLYFLON MG-6030 PTFE 15% Carbon Fiber Filled Molding Powder
15% carbon fiber filled. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechanical seals and bearing pads)Information provided by ..
Izod Impact, Unnotched 1.60 - 2.14 J/cm
3.00 - 4.00 ft-lb/in
Average value: 1.80 J/cm Grade Count:4
Overview of materials for Acrylic, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values o..
Izod Impact, Unnotched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 3003 Polymethylpentene (PMP), Glass Fiber
Izod Impact, Unnotched 1.60 - 7.47 J/cm
3.00 - 14.0 ft-lb/in
Average value: 3.76 J/cm Grade Count:34
Overview of materials for Polypropylene, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum ..
Izod Impact, Unnotched 1.60 - 5.34 J/cm
3.00 - 10.0 ft-lb/in
Average value: 2.76 J/cm Grade Count:7
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..
Izod Impact, Unnotched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 3001 Polymethylpentene (PMP), Glass Fiber
Copyright © lookpolymers.com All Rights Reserved