Mechanical Properties Metric English Comments
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 805 TFE 15 UV Acetal (POM), Glass Fiber Reinforced - PTFE Lubricated - UV Stabilized
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 807 Acetal (POM), Glass Fiber
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D 4812
RTP Company RTP PP 30 GF FR0 NAT Polypropylene (PP), Glass Fiber - Flame Retardant - Value Product - UL94
Flame Retardant - Glass Fiber - Value Product
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Europe-Africa-Middle East)
LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Heat Stabilized.
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 732E PBT + PC + PET
30% glass/mineral reinforced, excellent thermal performance, low shrinkage and warp. Easy flow.
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® DR48 PBT (Asia Pacific)
17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA.
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6/6 GF/M40 B1 BK 40% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearan..
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PES GF30 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP EC004XXC PEI (Asia Pacific)
LNP* Thermocomp* EC004XXC is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
Westlake Plastics Zelux® CN-P Polycarbonate (conductive)
Carbon-powder-filled with high flexural strength and good thermal stability to 275F. The CN-P is UL94 V-0 rated at 0.030" and is thermoformable in thinner gauges (0.010"-0.060").Information provide..
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 105 CC FR Polypropylene (PP), Glass Fiber - Chemically Coupled - Flame Retardant - UL94 V-0
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 1084 TFE 15 Polybutylene Terephthalate (PBT), Carbon Fiber - PTFE Lubricated
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 1305 TFE 15 Polyphenylene Sulfide (PPS), Glass Fiber - PTFE Lubricated
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 1378 Polyphenylene Sulfide (PPS), Glass Fiber - PTFE Lubricated
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 1481 TFE 10 Polyethersulfone (PES), Carbon Fiber - PTFE Lubricated
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.20 mm
10.0 ft-lb/in

@Thickness 0.126 in
ASTM D 4812
RTP Company RTP 203 C FR Nylon 11 (PA); Glass Fiber - Flame Retardant - 47% Renewable Resource Content
Renewable Resource Content calculated based on % of total compound weight.
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D 4812
RTP Company RTP 282 F Nylon 12 (PA), Carbon Fiber
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 299 A X 108950 A Nylon 6 (PA), High Gravity Compound
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 2100 TFE 10 Polyetherimide (PEI), PTFE Lubricated
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
Celanese FORTRON 1130L4 PPS, 30% Glass Reinforced
Fortron 1130L4 is a 30% glass-reinforced PPS that has excellent heat and chemical resistance. It is inherently flame-retardant and exhibits high hardness and a good balance of strength and stiffness..
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 203D  Nylon 6/12 (PA 6/12) Glass Fiber 20%  (discontinued **)
Glass Fiber 20%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.18 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Thermocomp® JF-1006 EM Polyethersulfone, Glass Fiber Reinforcement  (discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 3403-1 Liquid Crystal Polymer (LCP), Glass Fiber
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.20 mm
10.0 ft-lb/in

@Thickness 0.126 in
ASTM D 4812
RTP Company RTP 4799 X 117571 F Polytrimethylene Terephthalate (PTT) Glass Fiber - Flame Retardant - Halogen Free
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D 4812
RTP Company RTP 882 Acetal (POM), Carbon Fiber
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 1003 FR A Polybutylene Terephthalate (PBT), Glass Fiber - Flame Retardant - UL94 V-0
RTP 1001 - 1005 FRA are a series of glass fiber reinforced, flame retardant PBT compounds. All are UL94 V-0 certified down to the 1/32" (0.8mm) thickness. These materials exhibit easy flow, excellen..
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 200.5 A Nylon 6 (PA), Glass Fiber
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 302 TFE 15 Polycarbonate (PC), Glass Fiber - PTFE Lubricated
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 3503 Fluorinated Ethylene Propylene (FEP), Glass Fiber
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 987 Polysulfone (PSU), Carbon Fiber