Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.300 - 34.2 J/cm | 0.562 - 64.1 ft-lb/in | Average value: 2.28 J/cm Grade Count:88 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Izod Impact, Unnotched | 0.300 - 0.700 J/cm @Temperature 23.0 °C |
0.562 - 1.31 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 335/1 Rigid PVC, Extrusion Lead Free Profiles |
|||
Izod Impact, Unnotched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
Equate EMDA-8920 HDPE Injection Molding Resin EMDA-8920 is a high density copolymer polyethylene resin designed for injection molding applications which require excellent toughness and gloss.Applications: EMDA-8920 is a high density copolymer p.. |
|||
Izod Impact, Unnotched | 0.300 - 5340 J/cm | 0.562 - 10000 ft-lb/in | Average value: 0.300 J/cm Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |