Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.41 - 10.7 J/cm | 12.0 - 20.0 ft-lb/in | Average value: 8.45 J/cm Grade Count:13 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Izod Impact, Unnotched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256A |
LyondellBasell Higlass SB224-2 Polypropylene Copolymer, 20% Glass Fiber Key Features: conventional melt flow, medium modulus, chemically coupled, glass fiber-reinforced polypropylene copolymer, high impact strength, moderate rigidity, good processabilityApplications: of.. |
|||
Izod Impact, Unnotched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® PA6/6 CF30 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf.. |
|||
Izod Impact, Unnotched | 6.40 J/cm @Thickness 3.18 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with Un.. |
|||
Izod Impact, Unnotched | 6.40 J/cm @Thickness 3.18 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low .. |
|||
Izod Impact, Unnotched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PES GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 6.41 J/cm | 12.0 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® C-20 20% Calcium Carbonate-Reinforced Polypropylene Polifil® C series compounds are homopolymer polypropylene resins reinforced with fine particle size calcium carbonate. They combine high impact with stiffness, heat aging, good colorability, resist.. |
|||
Izod Impact, Unnotched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy E-17099B Nylon 6/6, Electrically Conductive - Carbon Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
Adell RZ-18 Copolymer Polypropylene, 40% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 6.40 - 9.60 J/cm @Temperature -40.0 - -40.0 °C |
12.0 - 18.0 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 8.00 J/cm Grade Count:2 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |