Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Glass Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.28 - 1.66 g/cc
0.0462 - 0.0600 lb/in³
Average value: 1.46 g/cc Grade Count:18
Filler Content 10.0 - 50.0 %
10.0 - 50.0 %
Average value: 29.1 % Grade Count:12
Water Absorption 0.200 - 0.300 %
0.200 - 0.300 %
Average value: 0.238 % Grade Count:4
Maximum Moisture Content 0.0200
0.0200
Average value: 0.0200 Grade Count:4
Linear Mold Shrinkage 0.000400 - 0.00300 cm/cm
0.000400 - 0.00300 in/in
Average value: 0.00157 cm/cm Grade Count:13
Mechanical Properties Metric English Comments
Hardness, Rockwell R 60.0 - 70.0
60.0 - 70.0
Average value: 66.3 Grade Count:4
Hardness, Shore D 55.0 - 83.0
55.0 - 83.0
Average value: 71.3 Grade Count:12
Tensile Strength, Ultimate 20.7 - 96.0 MPa
3000 - 13900 psi
Average value: 65.0 MPa Grade Count:14
Tensile Strength, Yield 52.4 - 79.3 MPa
7600 - 11500 psi
Average value: 63.6 MPa Grade Count:4
Elongation at Break 7.00 - 86.0 %
7.00 - 86.0 %
Average value: 23.1 % Grade Count:14
Elongation at Yield 15.0 - 35.0 %
15.0 - 35.0 %
Average value: 23.8 % Grade Count:4
Modulus of Elasticity 0.483 - 5.86 GPa
70.0 - 850 ksi
Average value: 2.85 GPa Grade Count:14
Flexural Yield Strength 15.2 - 116 MPa
2200 - 16800 psi
Average value: 66.6 MPa Grade Count:17
Flexural Modulus 0.345 - 5.85 GPa
50.0 - 848 ksi
Average value: 2.37 GPa Grade Count:18
Izod Impact, Notched 2.14 - 6.41 J/cm
4.00 - 12.0 ft-lb/in
Average value: 4.72 J/cm Grade Count:12
0.37373 - 1.81526 J/cm

@Temperature -40.0 - -40.0 °C
0.70015 - 3.40073 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.08 J/cm Grade Count:4
Izod Impact, Unnotched 6.41 - 5340 J/cm
12.0 - 10000 ft-lb/in
Average value: 12.8 J/cm Grade Count:4
Izod Impact, Notched (ISO) 11.0 - 76.0 kJ/m²
5.23 - 36.2 ft-lb/in²
Average value: 35.8 kJ/m² Grade Count:6
Izod Impact, Unnotched (ISO) 100 kJ/m² - NB
47.6 ft-lb/in² - NB
Average value: 109 kJ/m² Grade Count:6
52.0 - 95.0 kJ/m²

@Temperature -30.0 - -30.0 °C
24.7 - 45.2 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 75.0 kJ/m² Grade Count:5
Charpy Impact Unnotched 11.3 J/cm² - NB
53.8 ft-lb/in² - NB
Average value: 12.5 J/cm² Grade Count:6
8.70 - 103 J/cm²

@Temperature -30.0 - -30.0 °C
41.4 - 490 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 68.3 J/cm² Grade Count:6
Charpy Impact, Notched 4.00 - 7.90 J/cm²
19.0 - 37.6 ft-lb/in²
Average value: 5.30 J/cm² Grade Count:6
1.20 - 11.5 J/cm²

@Temperature -30.0 - -30.0 °C
5.71 - 54.7 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 3.27 J/cm² Grade Count:6
Taber Abrasion, mg/1000 Cycles 5.00 - 50.0
5.00 - 50.0
Average value: 21.7 Grade Count:6
Thermal Properties Metric English Comments
CTE, linear 13.5 - 55.8 µm/m-°C
7.50 - 31.0 µin/in-°F
Average value: 26.9 µm/m-°C Grade Count:10
Deflection Temperature at 0.46 MPa (66 psi) 51.0 - 199 °C
124 - 390 °F
Average value: 146 °C Grade Count:9
Deflection Temperature at 1.8 MPa (264 psi) 71.0 - 171 °C
160 - 340 °F
Average value: 131 °C Grade Count:13
Vicat Softening Point 79.0 - 182 °C
174 - 360 °F
Average value: 136 °C Grade Count:6
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+10 - 1.00e+15 ohm-cm
1.00e+10 - 1.00e+15 ohm-cm
Average value: 7.50e+14 ohm-cm Grade Count:4
Dielectric Strength 15.7 kV/mm
400 kV/in
Average value: 15.7 kV/mm Grade Count:3
Processing Properties Metric English Comments
Nozzle Temperature 221 - 243 °C
430 - 469 °F
Average value: 231 °C Grade Count:4
Melt Temperature 185 - 243 °C
365 - 469 °F
Average value: 218 °C Grade Count:8
Mold Temperature 15.6 - 60.0 °C
60.0 - 140 °F
Average value: 35.0 °C Grade Count:4
Drying Temperature 82.2 - 110 °C
180 - 230 °F
Average value: 99.0 °C Grade Count:8
Moisture Content 0.0100 - 0.0200 %
0.0100 - 0.0200 %
Average value: 0.0175 % Grade Count:4
Dew Point -40.0 - -17.8 °C
-40.0 - 0.000 °F
Average value: -35.8 °C Grade Count:8
Injection Pressure 48.3 - 103 MPa
7000 - 15000 psi
Average value: 79.2 MPa Grade Count:6