Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.85 J/cm @Thickness 3.17 mm |
14.7 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Triloy® 410 PC/PET alloy
(discontinued **) Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityGood flowApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang |
|||
Izod Impact, Unnotched | 7.85 - 5340 J/cm | 14.7 - 10000 ft-lb/in | Average value: 8.50 J/cm Grade Count:5 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Unnotched | 7.83 J/cm | 14.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP MX91206 PP LNP* Lubricomp* MX91206 is a compound based on Polypropylene containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched | 7.85 J/cm @Thickness 3.17 mm |
14.7 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Triloy® 170 PC/PBT alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityFlame retardantApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Izod Impact, Unnotched | 7.85 J/cm @Thickness 3.17 mm |
14.7 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Triloy® 215 PC/ABS alloy Characteristics:Dimensional stabilityHigh heat resistanceGood flowApplications:Camera partsExterior panelCluster fasciaWheel coverStructural applicationI/P. core panelHelmet shellGlove box doorCowl .. |
|||
Izod Impact, Unnotched | 7.85 J/cm @Thickness 3.17 mm |
14.7 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Triloy® 225 PC/ABS alloy Characteristics:Impact resistantHeat resistantDimensional stabilityApplications:Air con. grillAll information provided by Samyang |
|||
Izod Impact, Unnotched | 7.85 J/cm @Thickness 3.17 mm |
14.7 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3022L1 Polycarbonate, Lens Grade TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Izod Impact, Unnotched | 7.82 J/cm | 14.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RX09411H PA 66 LNP* Thermocomp* RX09411H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare. |