Polymer Property : Izod Impact, Unnotched = 5.34 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 385 TFE 10 SI 2 Polycarbonate (PC), Carbon Fiber - PTFE Lubricated - Silicone Lubricated
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 4082 AR 15 TFE 15  Polyphthalamide (PPA) Carbon Fiber 15% - Aramid Fiber 15% - PTFE 15%
Carbon Fiber 15% - Aramid Fiber 15% - PTFE 15%Comments:Carbon FiberAramid FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affe..
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D 4812
RTP Company RTP 800 AR 10 TFE 10 Acetal (POM), Aramid Fiber - PTFE Lubricated
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 800 AR 15 TFE 10 Acetal (POM), Aramid Fiber Reinforced - PTFE Lubricated
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D 4812
RTP Company RTP PP 30 GF FR0 NAT Polypropylene (PP), Glass Fiber - Flame Retardant - Value Product - UL94
Flame Retardant - Glass Fiber - Value Product
Izod Impact, Unnotched 5.34 J/cm

@Temperature 23.0 °C
10.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp FX00617 PE
LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Amer..
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics ULTEM 2110EPR PEI
10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 732E PBT + PC + PET
30% glass/mineral reinforced, excellent thermal performance, low shrinkage and warp. Easy flow.
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON EE004 PEI
LNP* STAT-KON* EE004 is a compound based on Polyetherimide resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON EE004 PEI (Asia Pacific)
LNP* Stat-kon* EE004 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PP GF/M40 CC BK 40% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP JF006E PES
LNP* THERMOCOMP* JF006E is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
Westlake Plastics Kynar® PVDF CN-F Polyvinylidene Fluoride (conductive)
Non-sloughing carbon-fiber-filled material with resistance to most chemicals and solvents mechanically strong and tough, thermally stable to 335F, flame and abrasion resistant, and easily fabricated..
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.20 mm
10.0 ft-lb/in

@Thickness 0.126 in
ASTM D 4812
RTP Company RTP 100 MF GB 20 UV Polypropylene (PP); Glass Beads - UV Stabilized
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.20 mm
10.0 ft-lb/in

@Thickness 0.126 in
ASTM D 4812
RTP Company RTP 1483 Polyethersulfone (PES); Carbon Fiber
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 199 X 108940 B Polypropylene (PP), High Gravity Compound
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 200 D TFE 20 Nylon 6/12 (PA), PTFE Lubricated
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 2383 C Rigid Thermoplastic Polyurethane (RTPU), Carbon Fiber
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D4812
A. Schulman SCHULAMID® 66 PTFE20 HS 20% PTFE Lubricated, Heat Stabilized Nylon 6/6
Information provided by A. Schulman.
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company EMI 961 Polysulfone (PSU), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 103 CC FR UV Polypropylene (PP), Glass Fiber Reinforced - Flame Retardant - UV Stabilized
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 203 D FR Nylon 6/12 (PA), Glass Fiber - Flame Retardant
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 203D  Nylon 6/12 (PA 6/12) Glass Fiber 20%  (discontinued **)
Glass Fiber 20%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 4005A FR  Polyphthalamide - Hot Water Mold (PPA) Glass Fiber 30% - Flame Retardant &a
Glass Fiber 30% - Flame RetardantComments:Glass FiberFlame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information ..
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company ESD A 1480 N  Polyethersulfone (PES) Dissipative - Carbon Fiber - High Viscosity &nbs
Dissipative - Carbon Fiber - High ViscosityComments:Static DissipativeESD ProtectionCarbon FiberHigh ViscosityUnless otherwise specified, all data listed is for natural or black colored materials. P..
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 1701 FR Modified Polyphenylene Oxide (PPO), Glass Fiber - Flame Retardant - Halogen Free
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 803 CC TFE 15 Acetal (POM), Glass Fiber Reinforced - PTFE Lubricated
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 804 SI 2 Acetal (POM), Glass Fiber Reinforced - Silicone Lubricated
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
RTP Company RTP 804 TFE 13 SI 2 Acetal (POM), Glass Fiber Reinforced - PTFE Lubricated & Silicone Lubricated
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
Celanese FORTRON 1130L4 PPS, 30% Glass Reinforced  (Unverified Data**)
Fortron 1130L4 is a 30% glass-reinforced PPS that has excellent heat and chemical resistance. It is inherently flame-retardant and exhibits high hardness and a good balance of strength and stiffness..