Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.20 - 5340 J/cm | 6.00 - 10000 ft-lb/in | Average value: 9.26 J/cm Grade Count:75 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Unnotched | 3.20 - 60.0 J/cm | 6.00 - 112 ft-lb/in | Average value: 8.89 J/cm Grade Count:34 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF5 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF60 BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® HDPE TM5 5% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 6.00 ft-lb/in | ASTM D256 |
Spartech Korad® SP-9071 FR/ABS Flame Retardant Sheet Description: Flame Retardant SheetKorad is a registered trademark of Polymer Extruded Products, Inc..Information provided by Spartech. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 CM30 L 30% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Composit.. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 6.00 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® T-20 20% Talc-Reinforced Polypropylene Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora.. |
|||
Izod Impact, Unnotched | 3.20 - 5.34 J/cm | 6.00 - 10.0 ft-lb/in | Average value: 4.76 J/cm Grade Count:7 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Izod Impact, Unnotched | 3.20 - 6.41 J/cm | 6.00 - 12.0 ft-lb/in | Average value: 4.34 J/cm Grade Count:4 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |
|||
Izod Impact, Unnotched | 3.20 - 11.7 J/cm | 6.00 - 22.0 ft-lb/in | Average value: 6.57 J/cm Grade Count:20 |
Overview of materials for Polyphthalamide (PPA), Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a.. |