Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Teknor Apex Company
Trade Name TELCAR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Specifications: Chrysler MS-DB590 CPN4062 Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
ASTM D955
0.013 cm/cm
0.013 in/in
ASTM D955
Melt Flow 2.00 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.00 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 42
42
10 seconds; ASTM D2240
Tensile Stress 8.41 MPa

@Strain 100 %
1220 psi

@Strain 100 %
2.0 in/min; ASTM D412
8.55 MPa

@Strain 300 %
1240 psi

@Strain 300 %
2.0 in/min; ASTM D412
Tensile Strength, Yield 7.58 MPa
1100 psi
Type 1, 20 in/min; ASTM D638
10.3 MPa
1490 psi
2.0 in/min; ASTM D638
Elongation at Break 140 %
140 %
20 in/min; ASTM D412
550 %
550 %
2.0 in/min; ASTM D412
Elongation at Yield 16 %
16 %
Type 1, 20 in/min; ASTM D638
Flexural Modulus 0.290 GPa
42.1 ksi
ASTM D790
Izod Impact, Notched NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D624
Gardner Impact 33.9 J

@Temperature -30.0 °C
25.0 ft-lb

@Temperature -22.0 °F
ASTM D3029
Tensile Impact Strength 470 kJ/m²
224 ft-lb/in²
ASTM D1822
>= 470 kJ/m²
>= 224 ft-lb/in²
ASTM D1822
Tear Strength 63.8 kN/m
364 pli
Die C; ASTM D1004
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 119 µm/m-°C

@Temperature -30.0 - 30.0 °C
66.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 117 µm/m-°C

@Temperature -30.0 - 30.0 °C
65.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 62.8 °C
145 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 40.6 °C
105 °F
Unannealed; ASTM D648
Glass Transition Temp, Tg -55.9 °C
-68.6 °F
DSC
Processing Properties Metric English Comments
Rear Barrel Temperature 171 - 193 °C
340 - 380 °F
Middle Barrel Temperature 177 - 199 °C
350 - 390 °F
Front Barrel Temperature 182 - 204 °C
360 - 400 °F
Nozzle Temperature 188 - 210 °C
370 - 410 °F
Zone 1 166 - 188 °C
330 - 370 °F
Zone 2 171 - 193 °C
340 - 380 °F
Zone 3 177 - 199 °C
350 - 390 °F
Zone 5 182 - 204 °C
360 - 400 °F
Die Temperature 190 - 210 °C
374 - 410 °F
Melt Temperature 188 - 210 °C
370 - 410 °F
Processing Temperature
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Back Pressure 0.172 - 0.345 MPa
25.0 - 50.0 psi
Cushion 0.381 - 2.54 cm
0.150 - 1.00 in
Screw Speed 50 - 100 rpm
50 - 100 rpm