Mechanical Properties Metric English Comments
Tensile Stress 8.40 MPa

@Strain 10.0 %,
Temperature 23.0 °C
1220 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR8685 BK022A TPC-ET  (Unverified Data**)
Hytrel® HTR8685 BK022A is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 44D, is pigmented black with fine particle size carbon black,..
Tensile Stress 8.41 MPa

@Strain 100 %
1220 psi

@Strain 100 %
2.0 in/min; ASTM D412
Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
Tensile Stress 8.41 MPa

@Strain 100 %
1220 psi

@Strain 100 %
2.0 in/min; ASTM D412
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
Tensile Stress 8.40 MPa

@Strain 100 %
1220 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® PL381-H TPC-ET
Injection Molding
Tensile Stress 8.40 MPa

@Strain 10.0 %
1220 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® PM460-H TPC-ET
Injection Molding, Heat Stabilized
Tensile Stress 8.40 MPa

@Strain 50.0 %
1220 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 8.42 MPa

@Strain 54.54 %,
Temperature 40.0 °C
1220 psi

@Strain 54.54 %,
Temperature 104 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 8.38 MPa

@Strain 37.22 %,
Temperature 120 °C
1220 psi

@Strain 37.22 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 8.40 MPa

@Strain 47.19 %,
Temperature 120 °C
1220 psi

@Strain 47.19 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 8.41 MPa

@Strain 134.13 %,
Temperature 120 °C
1220 psi

@Strain 134.13 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 8.40 MPa

@Strain 5.68 %,
Time 36000 sec
1220 psi

@Strain 5.68 %,
Time 10.0 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 8.40 MPa

@Strain 6.81 %,
Time 3.60e+6 sec
1220 psi

@Strain 6.81 %,
Time 1000 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 8.40 MPa

@Time 3600 sec,
Strain 4.98 %
1220 psi

@Time 1.00 hour,
Strain 4.98 %
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 8.40 MPa

@Strain 6.32 %,
Time 360000 sec
1220 psi

@Strain 6.32 %,
Time 100 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 8.40 MPa

@Strain 7.26 %,
Time 3.60e+7 sec
1220 psi

@Strain 7.26 %,
Time 10000 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 8.44 MPa

@Strain 0.400 %,
Temperature 60.0 °C
1220 psi

@Strain 0.400 %,
Temperature 140 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66  (Unverified Data**)
Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP..
Tensile Stress 8.40 MPa

@Strain 0.0400 %,
Temperature 40.0 °C
1220 psi

@Strain 0.0400 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)  (Unverified Data**)
60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo..
Tensile Stress 8.42 MPa

@Strain 0.310 %,
Temperature -20.0 °C
1220 psi

@Strain 0.310 %,
Temperature -4.00 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)  (Unverified Data**)
Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also..
Tensile Stress 8.38 MPa

@Strain 0.0400 %,
Temperature 23.0 °C
1220 psi

@Strain 0.0400 %,
Temperature 73.4 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..
Tensile Stress 8.44 MPa

@Strain 0.180 %,
Temperature 90.0 °C
1220 psi

@Strain 0.180 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610
30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Zytel RS 30G30L NC010 is a lubricated 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewabl..
Tensile Stress 8.40 MPa

@Strain 50.0 %
1220 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 4056P Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer in Powder FormInformation provided by DuPont Performance Polymers
Tensile Stress 8.40 MPa

@Strain 10.0 %
1220 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET  (Unverified Data**)
44 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Hytrel HTR8685 BK022A is designed for blow molding or processing techniques requi..
Tensile Stress 8.41 MPa

@Strain 100 %
1220 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G40D-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G40D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 8.41 MPa

@Strain 100 %
1220 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G40D-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G40D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..