Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® OBC 4530A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® OBC 4555A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® OBC 4665A Thermoplastic Elastomer Uses: Blow Molding Applications; General Purpose; Soft Touch Applications Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion;.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® OBC 4675A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL EF-6162 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1000-105 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1000-105UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1025-72 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; Closures; General Purpose; Grommets; Weatherstripping Forms:.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1140D BLK Thermoplastic Elastomer Uses: Automotive Applications; Automotive Interior Parts; Blow Molding Applications; Carpet Backing; General Purpose; Grommets; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injectio.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1431F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1686D Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1686D1 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1934A Styrenic Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Flexible Cord Jacketing; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL 1581Forms: P.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-1934C Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-2478K Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-2530F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-2540F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-2683A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-2717B Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Grommets; Industrial Soft; Sporting Goods; Toys; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injection Molding Inject.. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-3260R Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-3954-55 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-3954-90 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-4145A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-6800-73 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-83-F912-E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-83-F912-ER Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-93-T0488P-83 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-3954-45 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Zone 1 | 166 - 188 °C | 330 - 370 °F | |
Teknor Apex Telcar® TL-8732R Thermoplastic Elastomer Notes: RoHS Compliant Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstri.. |
|||
Zone 1 | 182 - 188 °C | 360 - 370 °F | |
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane Features: Excellent clarity and UV stable with good melt strength. Pre-drying: 2 hours at 104°C (220°F) in dehumidifying hopper dryerUses: Extrusion: Cable jacket, hose/tube, profile and film and .. |