Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® GC25A POM, 25% Glass Reinforced
(Unverified Data**) Celcon® acetal copolymer grade GC25A is a glass coupled formulation containing 25% reinforced fiber glass. This grade offers excellent strength, stiffness and heat distortion temperature with lower.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Celanese Hostaform® C 2521 LS POM, UV Resistant
(Unverified Data**) Stiff-flowing grade for injection molding and extrusion, UV resistantInformation provided by Celanese |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | Extrusion |
Kraiburg TPE THERMOLAST® K TC2TPN Thermoplastic Elastomer, General Purpose, Technical Performance The GP/AP Series is recommended for technical applications with excellent adhesion to PP. The compounds are available in natural and black colors. Typical applications:Function and design elements H.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | Extrusion |
Kraiburg TPE THERMOLAST® K TC4CSN Thermoplastic Elastomer, Optimized compression set The CS Series is recommended for sealing applications, providing an excellent compression set. The compounds are available in natural and black colors. Typical applications: FasteningsGrommetsMembra.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | Extrusion |
Kraiburg TPE THERMOLAST® K TP6HPG Thermoplastic Elastomer, Outdoor Grade Typical applications of the EX/UV Series: Edge guardsDistance ProfilesMolded Parts (Solar Equipment)SealsInformation Provided by Kraiburg TPE Corp. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | Extrusion |
Kraiburg TPE THERMOLAST® K TC7CSN Thermoplastic Elastomer, Optimized compression set The CS Series is recommended for sealing applications, providing an excellent compression set. The compounds are available in natural and black colors. Typical applications: FasteningsGrommetsMembra.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® OBC 4545A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL EF-6109 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-1431B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-2590A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-2625C Thermoplastic Elastomer Uses: Consumer Applications; General Purpose; Gaskets; Handles; Personal Care; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Ext.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-83-F912-E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-2470A Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-2545A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-97-T0214B-55 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Celanese Hostaform® C 13031 XF POM, Specialty Hostaform« acetal copolymer grade C13031 XF is an acetal copolymer modified to resist deterioration from aggressive fuel blends. This material is specially targeted for transportation industry fu.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Celanese Hostaform® C 2521 XAP² ™ POM, Unfilled POM copolymerInformation provided by Celanese |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Celanese Hostaform® C 52021 LS POM, UV Resistant POM copolymerInformation provided by Celanese |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Celanese Hostaform® MT12U03 POM, Medical Technology Hostaform« MT12U03 is a special grade developed for medical industry applications containing low residual monomers and no animal products. Hostaform« MT12U03 is a moderately high flow grade for fa.. |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® LM90Z POM, Specialty Celcon« LM90Z is a UV stable, nominal 9 melt flow acetal copolymer which is capable of being permanently marked by a laser. It gives protection against property and color deterioration in applicati.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Celanese Hostaform® C 13031 POM, Unfilled Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Hostaform® S 9243 XAP² ™ POM, Impact Modified POM copolymer, modifiedInformation provided by Celanese |
|||
Die Temperature | 190 - 220 °C | 374 - 428 °F | |
Celanese Hostaform® HS15 POM, Unfilled Drying is not normally required.Information provided by Celanese Corporation. |
|||
Die Temperature | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® GB25 POM, 25% Glass Reinforced
(Unverified Data**) Celcon® GB25 acetal copolymer is a 25% glass bead filled grade for low shrinkage and warp resistance in large, flat and thin walled parts.25% glass bead filled for stiffness, low warpageStandard re.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Celanese Hostaform® C 13031 XF POM, Specialty
(Unverified Data**) Hostaform® acetal copolymer grade C13031 XF is an acetal copolymer modified to resist deterioration from aggressive fuel blends. This material is specially targeted for transportation industry fu.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Celanese Hostaform® C 9021 GV1/20 POM, 20% Glass Reinforced
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMInjection molding grade, reinforced with ca. 20 % glass fibersInformation provided by Celanese |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Celanese Hostaform® C 13031 K POM, Tribological Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Celanese Hostaform® C 2521 G POM, Tribological Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Celanese Hostaform® C 27021 XAP POM, Unfilled POM copolymerInformation provided by Celanese |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Celanese Hostaform® C 9021 GV1/20 POM, 20% Glass Reinforced Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |