Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Polimeri Europa Europrene® SOL T 172 Styrene - Butadiene Block Copolymer
Europrene® SOL T 172 is a radial block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 30% weight. The polymer is extended with..
Specific Gravity 0.920 g/cc
0.920 g/cc
ISO 1183
Polimeri Europa Riblene® GM 20 Low Density Polyethylene - Coating Grade
Riblene GM 20 is a medium fluidity low density polyethylene resin (LDPE).Main Applications: Riblene GM 20 is suitable for coating applications where a low neck-in is required. Moreover, for its rh..
Specific Gravity 0.920 g/cc
0.920 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 121-65M300 Thermoplastic Elastomer  (discontinued **)
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and good..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
LTL Color Compounds ColorRxâ„¢ PE3-0200RX Biocompatible LDPE
A biocompatible Low Density Polyethylene for healthcare applicationsAll information provided by LTL Color Compounders, Inc.
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
LTL Color Compounds ColorRxâ„¢ PE3-0202ARX Biocompatible, Antimicrobial LDPE
A biocompatible Low Density Polyethylene for healthcare applications containing antimicrobial protection.All information provided by LTL Color Compounders, Inc.
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D4025
Kraton® D4150 K (SBS) Linear Block Copolymer
Description: Kraton D4150 K is a linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form identified: Kraton..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D4025
Kraton® G1701 H (SEP) Linear Diblock Copolymer
Description: Kraton G1701 H is a clear, linear diblock copolymer based on styrene and ethylene/propylene with a polystyrene content of 37%. It is supplied from North America in the physical form ide..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 45-LR-1 TPE
Product Description: StarTUFF TF 45-LR-1 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Teknor Apex Monprene® MP-1627I Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Teknor Apex Telcar® TL-1182A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Teknor Apex Telcar® TL-2507B Thermoplastic Elastomer
Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat..
Specific Gravity 0.920 g/cc
0.920 g/cc
Teknor Apex TruVis Esters™ DINA Di-Isononyl Adipate
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Teknor Apex UNIPRENE® 2005 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Westlake Plastics Propylux® 290 Polypropylene, Heat Stabilized
Through process improvement and advanced engineering, Westlake Plastics introduces the next generation of heat-stabilized polypropylene. Propylux 290 is produced from a FDA approved homopolymer res..
Specific Gravity 0.920 g/cc
0.920 g/cc
Zylog Hipolyene® 2703 MS Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
A. Schulman POLYBATCH™ Green 30394 Concentrate Based In LDPE
DescriptionPOLYBATCH® 30394 is a green color concentrate based in LDPE. This concentrate was designed to provide color in blow molding applications. POLYBATCH® 30394 is typically recommended for..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
A. Schulman POLYBATCH™ CE-505-E Concentrate Based In Polyethylene
DescriptionPOLYBATCH® CE-505-E is a 5% erucamide slip concentrate based in polyethylene. This concentrate is designed to reduce film COF in LDPE, LLDPE, and mPE cast and blown films. POLYBATCH® ..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D 792
RTP Company RTP 199 X 138789 EG Polypropylene (PP) Permanently Static Dissipative - ESD Protection - UV Stabilized - Extrusion Grade
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D 792
RTP Company RTP 299 A X 93036 B Nylon 6 (PA), Glass Bubbles
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Teknor Apex Telcar® TL-86-K986T-98 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Specific Gravity 0.920 g/cc
0.920 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 301 Ionomer
Information provided by A. Schulman.
Specific Gravity 0.920 g/cc
0.920 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 8221-85M300 Thermoplastic Elastomer
A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and ..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Dow TF0807 TPO
Dow Fascia TPO for Painted ApplicationsInformation provided by Dow
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
A. Schulman POLYBATCH™ Green 30394 Concentrate Based In LDPE
DescriptionPOLYBATCH® 30394 is a green color concentrate based in LDPE. This concentrate was designed to provide color in blow molding applications. POLYBATCH® 30394 is typically recommended for..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D 792
RTP Company RTP 2800 D-65A Thermoplastic Polyolefin Elastomer (TEO)  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Specific Gravity 0.920 g/cc
0.920 g/cc
foam molded; ASTM D792
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC1010 PPE+PS
LNP* Stat-kon* Noryl_FMC1010 compound is a 10% carbon fiber, static dissipative, foamable resin Nonchlorinated, nonbrominated. UL94 V1 rated. Property values at 20% WR, 0.250"" wall.
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Quadrant EPP Sanalite® PP, Homopolymer Polypropylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet)
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Kostat BK-STAT P048BK PP Sheet
BK-STAT Sheets are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness ..