Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.41 MPa @Strain 100 % |
1220 psi @Strain 100 % |
2.0 in/min; ASTM D412 |
Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Tensile Stress | 8.41 MPa @Strain 100 % |
1220 psi @Strain 100 % |
2.0 in/min; ASTM D412 |
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Tensile Stress | 8.41 MPa @Strain 134.13 %, Temperature 120 °C |
1220 psi @Strain 134.13 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.41 MPa @Strain 100 % |
1220 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G40D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G40D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 8.41 MPa @Strain 100 % |
1220 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G40D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G40D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |