Polymer Property : Die Temperature = 210 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Temperature 195 - 210 °C
383 - 410 °F
Extrusion
Stellarchem LP-880 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Die Temperature 190 - 210 °C
374 - 410 °F
Teknor Apex Telcar® TELC 302 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Die Temperature 190 - 210 °C
374 - 410 °F
Teknor Apex Telcar® TL-1000-105UV Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Die Temperature 190 - 210 °C
374 - 410 °F
Teknor Apex Telcar® TL-1427A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Die Temperature 190 - 210 °C
374 - 410 °F
Teknor Apex Telcar® TL-1686D1 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Die Temperature 190 - 210 °C
374 - 410 °F
Teknor Apex Telcar® TL-2507B Thermoplastic Elastomer
Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat..
Die Temperature 190 - 210 °C
374 - 410 °F
Teknor Apex Telcar® TL-2555A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Die Temperature 190 - 210 °C
374 - 410 °F
Teknor Apex Telcar® TL-2585A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Die Temperature 190 - 210 °C
374 - 410 °F
Teknor Apex Telcar® TL-2635C Thermoplastic Elastomer
Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi..
Die Temperature 190 - 210 °C
374 - 410 °F
Teknor Apex Telcar® TL-3260R Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Die Temperature 190 - 210 °C
374 - 410 °F
Teknor Apex Telcar® TL-4002 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Die Temperature 190 - 210 °C
374 - 410 °F
Teknor Apex Telcar® TL-86-K975-A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Die Temperature 190 - 210 °C
374 - 410 °F
Teknor Apex Telcar® TL-2270A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Die Temperature 190 - 210 °C
374 - 410 °F
Teknor Apex Telcar® TL-97-T0214B-55 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Die Temperature 170 - 210 °C
338 - 410 °F
Hotmelt Coating Slot Die
EMS-Griltech Griltex® 9E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Die Temperature 190 - 210 °C
374 - 410 °F
C 2521 XAP² ™ POM, Unfilled
POM copolymerInformation provided by Celanese
Die Temperature 190 - 210 °C
374 - 410 °F
C 9021 POM, Unfilled
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Die Temperature 190 - 210 °C
374 - 410 °F
C 9021 GV1/20 XGM POM, 20% Tribological  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMlow wear, 20% fiberglass reinforced, PTFE containing gradeInformation provided by Celanese
Die Temperature 190 - 210 °C
374 - 410 °F
C 9021 M XAP²™ POM, Tribological  (Unverified Data**)
POM copolymerwith molybdenum disulphide modified, low emissionInformation provided by Celanese
Die Temperature 199 - 210 °C
390 - 410 °F
Zone 1
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane
Features: Excellent clarity and UV stable with good melt strength. Pre-drying: 2 hours at 104°C (220°F) in dehumidifying hopper dryerUses: Extrusion: Cable jacket, hose/tube, profile and film and ..
Die Temperature 190 - 210 °C
374 - 410 °F
C 13031 K POM, Tribological
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Die Temperature 190 - 210 °C
374 - 410 °F
C 9021 GV1/20 XGM POM, 20% Tribological
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Die Temperature 190 - 210 °C
374 - 410 °F
LX90GC15 POM, 15% Specialty
Preliminary Data SheetInformation provided by Celanese
Die Temperature 190 - 210 °C
374 - 410 °F
MT24U01 POM, Medical Technology
« MT24U01 is a special grade developed for medical industry applications containing low residual monomers and no animal products. « MT24U01 is a low melt viscosity for fast cycling, thin walled in..